Hey all,

I need some help adjusting this glaze, because I need to substitute G200 hp for the custer feldspar. Would I adjust by adding +3 silica?

Please chime in with opinions.

Thanks,

juli

Maggie Moo's Blue-Green glaze Cone 6

From http://umtclayandglaze.blogspot.nl

Maggie Moo's Blue-Green glaze #5

This glaze recipe is adapted from a combination of a Mastering Cone 6 Glazes base glaze and Maggie Schlebecker's blue-green glaze recipe. It is cone 6 oxidation.

You can adjust the percentage of copper, tin, and zinc to produce a range of color from a pale mint to a deep sea green. Varying the amount of tin and zinc will affect the opacity of the glaze and make it milkier the more you add. Overdoing it on the copper could cause leaching, so going over 5% is probably not a good idea, but otherwise this base is extremely stable and food safe.

Custer Spar 20.0 (kaliveldspaat)

Ferro Frit 3134 20.0
Wollastonite 10.0
EPK 21.0 (kaoline)
Talc 11.5
Silica 17.5 (kwarts 
SiO2)
------------
Total 100.0

Add 

Tin Oxide 3.96
Zinc Oxide 2.45
Copper Carb 3.21 (or Black Copper Oxide 2.14)

Views: 3627

▶ Reply to This

Replies to This Discussion

My analysis shows them so close that it does not matter.  3% would be too much - 1% more would be good enough.

Using G-200HP feldspar, instead of Custer, replaces 2.1% Na flux with K flux, and increases total Na/K flux by 8%. I've found this direct replacement usually leads to brighter colors with less expansion.

Custer feldspar does have 3% more silica, but I wonder if you could tell the difference between a batch without an extra 3% silica and a batch with 3% extra silica.

Thanks for the helpful info all, I will test it this week.

juli

FYI - Feldspar comparison from Insight-Live 

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service