Steven Hill Oxidation Project
Achieving atmospheric glaze effects in electric kilns at mid-fire temperatures, through the layering of sprayed glazes. The starting point recipes are given in two discussions "Strontium Crystal Magic . . ." and "The Companion Glazes"
Joseph Fireborn
Makes perfect sense. Glad I questioned this. I have saved several hours in the last week no longer using this part. Although my entire schedule is a lot different than his.
May 13, 2017
Tom Anderson
Tom
May 13, 2017
Tom Anderson
This is the easiest and best resource for the various temperatures potters need to be concerned with.
http://www.quartzpage.de/gen_mod.html
Tom
May 14, 2017