Forum Discussions (387)

Discussions Replies Latest Activity

Glazing inside large pots

I'd normally pour the glaze for the inside of a pot, but I've made a couple of biggies - 17" tall, 12" diameter, the aperture at the top is…

Started by Ayjay in Glazes - Application Techniques

3 Aug 2, 2018
Reply by Ayjay

Pin holing -Revised Sapphire Blue Glaze

I've having major pin holing issues with  the Sapphire blue (revised) glaze recipe from Ron Roy's web site Frog Pond Pottery. It's happenin…

Started by Juanita Short in Glazes - Testing and Reporting

9 Jul 20, 2018
Reply by Juanita Short

Stars

Beyond the Market Tent to a Rolling Showroom

We have done festivals and various types of street shows using a very good Flourish Tent furnished with shelving to display the work. As an…

Started by Marla Stroup in Marketing & Business Savvy

7 Jun 9, 2018
Reply by josi rica

Online Glaze Calculation and Theory

Max Katz of Alfred University runs interactive 3 month classes in his understanding glaze materials workshop. You can watch some of his vid…

Started by George Lewter in Glazes - Theory and Chemistry

0 May 19, 2018

Stars

Tin Oxide substitutes

Has anyone been successful substituting Zircopac for Tin Ox in WARM JADE?

Started by Brenda B Hardt in Glazes - Recipe Exchange

5 May 8, 2018
Reply by Norm Stuart

Pete's Weathered Bronze (Green)

Recipe Name:  Pete's Weathered Bronze Cone:  6-9     Color:  green bronzeFiring:  Oxidation     Surface:  Matte Amount     Ingredient60    …

Started by George Lewter in Network User Guide

17 May 2, 2018
Reply by Barbara Hanselman

diamond discs

Hello everybody, I am looking for a   diamond disc  to put on the potter's wheel, here in Belgium I can't find it  or even in Europe . I w…

Started by josi rica in Network User Guide

11 Apr 23, 2018
Reply by josi rica

Raw glaze recipe

Hi, I've been trying to work out a raw glaze recipe, after reading a few books suggesting ball clay works better for raw glazing leather ha…

Started by Tom Humphries in Glazes - Theory and Chemistry

5 Mar 17, 2018
Reply by Tom Anderson

Firing with Cornstarch on the Clay Surface

I like to use cornstarch with my classes to keep my flexible rubber stamps from sticking to the clay surface but a kiln tech at one of my a…

Started by Barbara Hanselman in Firing Techniques

6 Mar 4, 2018
Reply by Barbara Hanselman

Stars

Glazes that break over images well

Wondering which  glazes "break" best over graphics etc. The mug displayed is an example, though it is not my own.   Do we achieve this with…

Started by cp dunbar in Network User Guide

2 Feb 26, 2018
Reply by Norm Stuart

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service