Forum Discussions (387)

Discussions Replies Latest Activity

Stars

Fake Ash Glaze Testing Help

Ron Roy has asked me to test some fake ash glazes to see if he can develop a fake ash that does not have pinholes or any bubbles.   If any…

Started by Randy McCall in Glazes - Testing and Reporting

12 Mar 7, 2011
Reply by susan claysmith

Glaze Simulator Dot Com

This Website has glaze calculation software that you can use free online.  Thank you, Zoophagous, for mentioning it on your blog. Here is t…

Started by George Lewter in Glazes - Development and Adjustment

7 Feb 24, 2011

Stars

Labeling Photos

I have said this long before and i think that it needs repeating.  It would help all of us if the photos that are posted gave some informat…

Started by eleanor akowitz in Network User Guide

7 Feb 22, 2011
Reply by pauline purdum

Electric Reduction Is Alive & Well - Though Not Yet on Main Street

Terry Fallon says it is doable and you can get 200 firings on a set of elements.  I had never heard of it (other than sagger firing) until…

Started by George Lewter in Firing Techniques

16 Feb 19, 2011
Reply by Nicholas Friedman

A Question of Kaolins from Mary Jane

At 12:40pm on December 23, 2010, Mary Jane said… Hi George - Another question.  The recipes I got at the Steven Hill workshop just say kao…

Started by George Lewter in Glazes - Theory and Chemistry

3 Dec 28, 2010
Reply by Mary Jane

Stars

Craters & pinholes

I do a lot of layering, sometimes good, sometimes not so good.  I usually do tests on a tile first & then pick a few combos & put t…

Started by Jeff Poulter in Glazes - Development and Adjustment

25 Dec 3, 2010
Reply by Ceci

Sources of Glaze Recipes

As a starting point, here is a list of online sources of cone 6 glaze recipes. It has been moved over from its former page, to help organiz…

Started by George Lewter in Glazes - Testing and Reporting

1 Jun 18, 2010

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014