Forum Discussions (387)

Discussions Replies Latest Activity

micro-crystalline glaze for c6

Hello everyone, I am trying to find a recipe for a crystalline glaze with small but well-visable cristals for c.6 Prefeable without barium.…

Started by marlies bontenbal in Glazes - Recipe Exchange

5 Oct 7, 2012
Reply by Steve Tyler

Vanadium

I want to try a 72 Base variation that calls for Vanadium. Unfortunately, it isn't clear whether that means pentoxide, oxide-- or even just…

Started by Shine Chisholm in Glazes - Recipe Exchange

4 Oct 6, 2012
Reply by Shine Chisholm

Ceramics Conferences

Have you been to any  ceramics conferences?  What is good or bad about them and how do they compare to workshops. 

Started by George Lewter in Continuing Education

2 Sep 22, 2012
Reply by Nadine Mercader

Stars

An Enjoyable 'Raku Firing Day' in Australia

Despite and extremely windy Spring afternoon here in Australia yesterday, Rhonda Morris and I had a very enjoyable and successful raku firi…

Started by Jan Wallace in Firing Techniques

1 Sep 12, 2012
Reply by Wally Wallace

Stars

Spraying ash glazes

Group,  I just unloaded the kiln with a few more pots using ash glazes.  Cone 6 purchased glazes.  Sprayed with atomizer (by mouth).  They…

Started by June Kinsinger in Network User Guide

5 Aug 21, 2012
Reply by Brian Guffey

Stars

Web presence?

A study group/course I would be very interested in is one about creating a web presence, particularly creating a web site.  Anyone else and…

Started by Kathy Ransom in Continuing Education

7 Aug 14, 2012
Reply by Brian Guffey

Glazing the Foot (From Joanna Turnbull)

Joanna said on July 24, 2012: "I am fairly new to pottery and would really love to know how one goes about glazing a piece so that there is…

Started by George Lewter in Glazes - Application Techniques

8 Aug 6, 2012
Reply by Brian Guffey

Cone6pots World Raku Party

Suggested date - August 11, 2012 Location - Multiple regional locations around the globe. Objective - Meet and enjoy time with other C6P me…

Started by George Lewter in Workshops, Conferences, Seminars

10 Jul 24, 2012
Reply by George Lewter

I'd like some help learning to fire an Evenheat 4320 with kiln sitter...

I bought a used Evenheat 4320 kiln with kiln sitter.  It does not have knobs to adjust heat settings.  I has 4 switches that you turn on on…

Started by Renee Arthur in Network User Guide

7 Jul 14, 2012
Reply by Renee Arthur

Attaching handles and other appendages to moist clay.

This is a compilation of a string of comments in the S Hill Ox Project group area, brought here as the basis for a discussion. Comment by T…

Started by George Lewter in Altering and Decorating Forms

1 Jul 13, 2012
Reply by Denise S Morris

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by