Forum Discussions (387)

Discussions Replies Latest Activity

Stars

Witness Cones always indicate one cone hotter than Bartlett Controller V6-CF

Has anyone compared their computerized Kiln Controller and thermocouple cone with Witness Cones? Witness Cones in our computer-controlled k…

Started by Norm Stuart in Firing Techniques

4 Mar 13, 2013
Reply by Norm Stuart

Transparent glaze

A recipe for transparent jade green was given by a member about a year ago.    It's a beautiful and working glaze that I enjoyed using unti…

Started by Nancy Bibby in Glazes - Recipe Exchange

0 Mar 4, 2013

drippy cone 6 glaze

Hello,  I'm looking for a cone 6 base glaze recipe that is not just runny but will give nice big fat drips.  I'd like to use this glaze as…

Started by Grace Sheese in Glazes - Recipe Exchange

1 Feb 4, 2013
Reply by Brian Guffey

Where do you sell your ceramic work.

Currently I am trying to build up enough items so I can have some semblance of a "store" when I start selling. Most potters I meet, scoff a…

Started by George Lewter in Marketing & Business Savvy

18 Jan 31, 2013
Reply by Brian Guffey

Online Glaze Recipe Database Project is Now Under Way

Tony Hansen, owner of the Digitalfire Corporation contacted me after my  announcement went out that we were about to develop an online glaz…

Started by George Lewter in Glazes - Testing and Reporting

15 Jan 20, 2013
Reply by June Perry

A glaze spraying tutorial, online, in pdf form

Here is a link to a wonderful glaze spraying booklet produced by an Aussie, Roger Graham. It contains references to Australian companies, m…

Started by Belinda Willis in Glazes - Application Techniques

9 Jan 7, 2013
Reply by George Lewter

Gerstley Borate / Kona F4 Feldspar and substitutions

I just started making my own glazes again this year. Before that, it had been about ten years. At that time, Gerstley Borate and Kona F4 Fe…

Started by Shine Chisholm in Glazes - Theory and Chemistry

5 Dec 28, 2012
Reply by Shine Chisholm

Stars

warping platters

Hi All I fired a student's oval platter (cone 6) on triangular stilts.  It warped, I think because I placed the stilts incorrectly. I was t…

Started by Donna Ferrara in Firing Techniques

2 Dec 23, 2012
Reply by Donna Ferrara

Need some engobe help please.

Hi everyone! I've been working with clay for a little over a year now and my husband and I have decided that commercial glazes are becoming…

Started by Dora Anderson in Glazes - Application Techniques

5 Dec 21, 2012
Reply by Kabe Burleson

Looking for a good clear glaze for little loafers

Im considering switching my clay to little loafers. I need to find a good clear glaze to go over slip decorations. I'm going to test what…

Started by Leigh Whitaker in Glazes - Recipe Exchange

5 Dec 16, 2012
Reply by Leigh Whitaker

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service