PA Frogskin Glaze

I am not certain of the origin of this glaze but I got it from the Prince Albert Arts Center and I believe they got it from the Saskatoon P…

Started by Kathy Ransom in Glazes - Recipe Exchange

22 Apr 11, 2014
Reply by Norm Stuart

Porosity Problems

Hi Everyone,I've been potting for about 4 months, mainly wheel throwing. I've had successes and failures but apart from my first glaze firi…

Started by Jeff Morfett in Firing Techniques

4 Apr 1, 2014
Reply by Nadine Mercader

red pink purple mauve glaze

I saw this glaze at a crafts fair.It was beautiful and breaking to all of those colors. I have since tried it and I get a rather ordinary l…

Started by Lawrence Weathers in Glazes - Development and Adjustment

1 Mar 30, 2014
Reply by Wyndham Dennison

Stars

CuO3

So I have a recipe that calls for the above.  Upon searching you come up with various answers, but the bottom line is that it is copper oxi…

Started by Jeff Poulter in Ceramic Materials Education

3 Mar 28, 2014
Reply by Norm Stuart

Stars

Alberta Slip II

I was reading on Pottery.About.Com that Albany Slip II is really Ravenscrag Slip & I was thinking that that just doesn't sound right.  …

Started by Jeff Poulter in Ceramic Materials Education

2 Mar 28, 2014
Reply by Jeff Poulter

Orton: calculation spreadsheet

attached is a :cone calculation Excell spreadsheet that I got from a guy at Orton, but is not on their website.. It is pretty slick and I t…

Started by Lawrence Weathers in Firing Techniques

1 Mar 27, 2014
Reply by Norm Stuart

From raku to stoneware

Hi every one, I have a dilema. I have been producing this lotus pattern with Raku quite successfully.I would really like to be able to do t…

Started by Jennifer Arthur in Glazes - Application Techniques

4 Mar 27, 2014
Reply by Jennifer Arthur

Stars

Magic Water for slip

Magic Water is described as a means of joining two pieces of greenware or attaching handles that have broken off as well as closing cracks.…

Started by Marla Stroup in Altering and Decorating Forms

6 Mar 24, 2014
Reply by Nadine Mercader

Stars

Issues with Jen's Juicy Fruit - Only problem glaze in a full load of tests?????

I would appreciate some feedback re this Jens Juicy fruit glaze I tested the other day. I fired a kiln load of tests with success EXCEPT fo…

Started by Jan Wallace in Network User Guide

11 Mar 24, 2014
Reply by Ayjay

Slip Glazes

Slip glazes are glazes developed from natural materials that might be usable as clays in a low fire range, but actually melt down and becom…

Started by George Lewter in Glazes - Development and Adjustment

4 Mar 19, 2014
Reply by George Lewter

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service