Forum Discussions (387)

Discussions Replies Latest Activity

Stars

Chinese Brush Painting

which brushes do you use, where do you get them, any books you know of to help ?

Started by cp dunbar in Glazes - Application Techniques

1 May 1, 2014
Reply by George Lewter

Stephen Hill firing schedule

One unique feature of Stephen Hill's firing schedule is that he goes to someplace in ^ 5 then holds for up to an hour until the ^ 6 drops. …

Started by Lawrence Weathers in Firing Techniques

4 Apr 25, 2014
Reply by Lawrence Weathers

Feldspar Question

I am planning on trying out some new glazes this week.  I came across the Gartside base.  It calls for "Feldspar, G-200."  Isn't the G-200…

Started by Chantay Poulsen in Glazes - Theory and Chemistry

3 Apr 21, 2014
Reply by Chantay Poulsen

Stars

How to interpret this recipe for Lynn's Glossy Gray-blue green

I am trying to mix the recipe that is the glaze on Barbara Hanselman's  'Egyptian Bowl'. Gerstly borate     50 Silica                   3…

Started by martha peddicord in Glazes - Testing and Reporting

1 Apr 19, 2014
Reply by Wyndham Dennison

Should We Start Our Own Ceramic Art and Craft Online Market Place

Some of our members use etsy, or other online craft mall. Some have their own websites for marketing their own work. On the craft malls, it…

Started by George Lewter in Marketing & Business Savvy

9 Apr 16, 2014
Reply by Lawrence Weathers

Chemistry in Ceramics

I made a PowerPoint presentation for lectures I gave. It is too big to attach here (16,7 MB), but you can find it on my website: Chemistry…

Started by Daniel Spruyt in Glazes - Theory and Chemistry

2 Apr 16, 2014
Reply by Daniel Spruyt

Keeping record of your work

OK, I give it another try...Integrated in my database mentioned before, I developed a system to evaluate glazes and it can - to some extend…

Started by Daniel Spruyt in Glazes - Testing and Reporting

2 Apr 16, 2014
Reply by Daniel Spruyt

how thick should your glaze be sprayed on and how do you tell if it is that thick?

I'm getting tired of the common "hose and hope" strategy. in Mastering Cone 6 Glazes they point out that one of the most difficult things…

Started by Lawrence Weathers in Glazes - Application Techniques

13 Apr 14, 2014
Reply by Jennifer Arthur

Keeping record of your work

If you use many different glazes or always try new ones like me, it is important to keep record of everything you do. To do so I use the re…

Started by Daniel Spruyt in Glazes - Testing and Reporting

0 Apr 13, 2014

Slipcast molds available for sale through eBay

Hi guys, A recently deceased relative left several ceramic slipcast molds, most of which were stored in handmade wooden boxes for the past…

Started by Shine Chisholm in Pottery Equipment

0 Apr 12, 2014

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service