Firing to cone 6 twice in the same firing?

Started this discussion. Last reply by Pat Jun 28, 2016. 14 Replies

So I have a curious question for all you cone 6 firers out there. I recently refired a few pots and the glaze was completely free of microdimples. I have really good surfaces on most of my glossy…Continue

Spraying Glazes - A good starter compressor and spray gun set?

Started this discussion. Last reply by Joseph Fireborn Dec 26, 2015. 2 Replies

I see a lot of beautiful work done by people spraying glazes. I have only been brushing and dipping for a long time now and I am ready to move into a new way to decorate pots.I purchased the Stephen…Continue

Tags: glazes, spray

 

Joseph Fireborn's Page

Profile Information

What is your experience with ceramics in general. (Long answer encouraged)
I am a garage potter. Been potting for a little over three years.

Exploring the beautiful surfaces of porcelain with sand and grog. 99% of my work is testing to develop my personal aesthetic.
What is your current involvement with electric fired ceramics? (long answer encouraged)
I fire 2-3 times a week in my kiln. Constantly adapting glazes and modifying them using insight live.
All our content is viewable by the public. Why do you want to be a member, when you can already see everything as a non-member?
So I can contribute and converse.
Where do you work on your ceramics projects?
home studio
Do you have your own, or participate in other ceramics Websites:
http://josephmakespots.com
How did you find this network?
search engine

Joseph Fireborn's Photos

  • Add Photos
  • View All

Comment Wall (1 comment)

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

At 8:50pm on February 11, 2016,
Stars
Erik Evans
said…

Sir, 

Nice work.  Really.  You've got some fairly standard cone 6 glazes working for you, in your own way.  That's not so easy.   The extra effort you make to tweak recipes and spray your glaze is paying off.  Stand-out work.  Nice job.  Keep it up!     

 
 
 

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service