I finally have the glazes mixed from the March workshop I took with SH.  I would like to fire SH glazes in the same kiln with MC6G that I have been using successfully.  The cooling rates are very different.  I used the scedule SH gave us and the MC^6 glazes came out glossy, where with Hessleberth's firing recommendations, they are nice matts and satins.  SH says if strontium glazes are cooled too slowly they are rough.

 

Anyone??

Views: 1315

Replies to This Discussion

Hi June. I'm not Martha but I can answer about SCM W. The W is for Warm and produces a warmer recipe due to inclusion of RIO in the recipe. It also has other adjustments. I am on the road and don't have the recrecipe at hand. Maybe someone else can share.

John Lowes

Thanks John. I hope someone else will post the recipe if you don't.

I'm starting to weigh out some of those test glaze batches today, now that all the tiles are made and drying.

The recipe I use for warm colors is SCMO (SCM for Orange) and I got it from this page:

http://www.flickr.com/photos/searleb/sets/72157603557658326/

It's the same recipe as SCM plus 2% Yellow Iron Oxide. If there's a version with RIO that works better in oxidation, I'd be interested in hearing about it too.

Have you tried it with the 2% red iron oxide in oxidation? The intensity would be increased if you use a very high quality red iron oxide that is available through some suppliers, or just add a bit more of your regular iron oxide if it's not as intense as you would like. I doubt if you'd get orange in oxidation with only 2% red iron.

Some high purity red iron oxides have a 99% purity. Georgies in Portland has one that is high purity but they don't mention the percentage. Bailey's has one that is 93% purity. I don't know how those compare to Spanish red iron.

High alumina  matts with 8% rutile and 4% tin oxide will give a strong orange (I have a recipe and photo in one of my cone 6 test tile groups on my web page).Here's my recipe if you want to try it. I didn't fire it down, so I don't know what it will do, but it was very nice just tested in my small test kiln.

 

June Perry #7473 V3 color A. It is another calcium eutectic type glaze. It has a lovely surface and medium peach color, darker than the one next to it. Tile is porcelain.

Recipe:

25.23 Custer Feldspar

40.92 Wollastonite

20.28 EPK

4.13 Calcined Kaolin

0.18 Talc

9.27 Silica

Total 101

M colors ADD: Rutile 8%, Tin oxie 4%

 

This is a good matt, and I would imagine if you use the Steven Hill or similar firing cycles, it would work well, since the high calcium with that kind of firing schedule may benefit the crystal growth. 

On my web site there are a few variations of this base glaze with lower amounts of rutile for peach tones.

 

June

http://www.shambhalapottery.com

http://www.shambhalapottery.com

 

 

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service