Everyone has experienced this - Not all of our glazed pots are pleasing .....We unload our glazed pots from a warm kiln with the excitement of a 5 year old- waiting to get down to that shelf which holds the one piece we really want to see......and Yeck - there it is. Not what we planned, perhaps even ugly. Sometimes it's just a flaw that makes it unusable/ un-sellable, a tiny spot that we missed glazing or a drip that dripped too far.

I sell my work so salvaging a piece means more than just liking it- it means potential revenue lost. But regardless of the final resting place of your work - we all like to salvage our mistakes.

Reglazing is a tricky business. In the studio where I teach I try to get my students to understand that it's a risk to reglaze and that the piece may very well be even worse off. Existing glaze remelts and moves, warpage and blistering can occur, and other over fired looking effects can overcome.

I tell my students it's a waste of kiln space and glaze to refire/reglaze a piece that only your mother would like - so be sure it's a worthwhile piece to begin with. Sometimes I have found great new combinations by mistake in the process of reglazing though. That said.

The Application of new glaze - Heat the pot up - microwave- heat gun - whatever will get it hot. Then reglaze it. This makes the new wet glaze dry quickly on the surface and adhere better. If it's just a small spot you need to heal then feather the glaze in over the area. If it's a dip - then be sure to have a nice big fat clearance at the bottom so it doesn't run to the base. Sometimes I put those pieces on a biscuit, depending on how close the first glaze came to the base. 

Heat Helps- Reglazing can be a Risky Business.

Views: 7977

▶ Reply to This

Replies to This Discussion

Ancient jasper needs to be thick! And not over fired I use it a lot Also never fire in gas it turns a disgusting purple. I've had good luck with palladium but I mostly use it on top of other glazes. And on the top portion as it runs
I apply three thick coats but every piece I have used it on comes out black with small variances here and there. Have not been pleased with any results yet

Sometimes on a refire, one is emboldened to try something really different, particularly on a pot that is a total loss, such as the following.

This is the way my single fired mug came out of a reduction firing. The glaze (Malcom Davis Shino) was not able to bond to the raw B-mix 5 clay. It shrank more in the firing than the body and the poor bond caused crawling more than crazing. The glaze was also not completely melted, accounting for the flakes. In thinking about refiring the pot, I knew that I was going to need a very fluid glaze to penetrate the cracks and voids in the shino, and to adhere the flecks of shino firmly to the body. The first step was to knock down and remove curled flecks of shino that were standing in high relief, particularly around the rim where someone might want to put their mouth. I did that by tapping on those areas with the wooden handle of a hammer to break off all the projections and loose pieces. I then dipped the mug in heavy cream consistency Floating Red glaze, dried it with a heat gun, dipped it again, dried it, and after cleaning the bottom off, it was ready to fire to cone 6 in my electric kiln. 

I was very lucky with my choice of Floating Red as a covering glaze. I've seen other glazes behave horribly on top of true shinos. The finished product totally exceeded my expectations, flowing nicely into and accentuating all cracks and voids, and flowing gracefully down the chattered texture in the middle of the mug. Part of the rim was still rougher than I wanted for mouth contact, so I used a diamond grit sanding block and fine wet/dry carbide sanding paper to smooth it. The rim is now smooth enough for even my tender lips.

There is an excellent set of glaze application tips --- Glazing for Success: 12 Tips to Help You Master Pottery Glazing from Annie Chrietzberg posted on Ceramic Arts Daily. If you suffer a lot of glaze defects, it is highly likely that one of these factors is the culprit. I give this article five stars.

I tried reglazing once by preheating the piece. I still couldn't get the glaze to stick right. I also tried the hair spray trick. After that I decided non of my pieces were worth that headache! What trips me, is that when a pot comes out "wrong" and I absolutely hate it, someone else loves it. I throw pieces away that crack, or have flaws that would make the piece useless but rarely for glaze. Even if it shivers off the piece someone thinks that is cool. Sometimes we need to look at the piece differently.

I want to share that before starting the process of reglazing (very rarely) with the heating of the piece, I always degrease its surface (finger prints) wiping it with a cloth soaked with cellulosic thinner or dichloromethane (dry cleaning solvent, much more efficient and...toxic)

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service