Just want to say thank you to all the people who have shared glaze recipes! I have tested many, and just wanted to show and tell!

Views: 854

Attachments:

▶ Reply to This

Replies to This Discussion

Beautiful work Juli! You should post these in your images.

I have this at a small gallery where I live. The white pots glaze is "Donna's Matte white base", the green pitchers on the top are modified xavier over metallic green. Top shelf, maggie moo on teapot and mugs, and teapot has maggie moo over nutmeg, and some of the pitchers and teapot on the fourth shelf are maggie moo over nutmeg.  Second shelf is xavier over metallic green over nutmeg.  I could not have done this without your help, so thank you so much!!!!

la paloma texas pottery

juli long

Thanks Nadine

It took me forever to get these posted, and I see they didn't show up. shit, I will try your suggestion! Thanks again for the compliment!



Nadine Mercader said:

Beautiful work Juli! You should post these in your images.

I love the green on the pitchers.  Is that Xavier's warm Jade?  I have seen that elsewhere, but the potter did not have the  recipe, she was working out of a co-op with their glazes.  Are you willing to share?    It looks a lot like one I have called SEAFOAM , but the green is brighter, more grass color in what you have.  Beautiful.

Martha,

Sharing is how I got these recipes!!   To get that grass green, I layer two glazes, I sometimes do one over the other and vice versa.  The xavier, and metallic green.  recipes below.  

Revised Xavier warm jade green   (food safe)

G200 HP  22

frit 3134    16

Whiting     12

talc           9

Epk          20

Silica        21

copper carb     3

rutile        5

metallic green  (not food safe)

frit 3269    27

Gillespie borate   15

spodumene     40

epk      18

add

tin  ox       6.8

copper carb    4.8

Thank you.  I will mix and test soon.  I have been looking for a more true green for a while.


 Is the rutile dark or light?  I just recently learned that it can make a difference.

Martha,

Sorry, I have no clue.  I just order rutile.

Juli

martha peddicord said:


 Is the rutile dark or light?  I just recently learned that it can make a difference.

Is yours the color of a brown paper grocery bag, or darker, with a more mocha, coffee with just a bit of cream   I have both and it does make a diff.

I can ,mix either way, just wondering .

Martha,

Its grocery bag brown.  Im gonna start calling it that now.



martha peddicord said:

Is yours the color of a brown paper grocery bag, or darker, with a more mocha, coffee with just a bit of cream   I have both and it does make a diff.

I can ,mix either way, just wondering .

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014