Comment by Denice E. Demuth on March 3, 2014 at 9:24pm

Thank you for the White Crawl Glaze formula, I know how much trouble you went to.  I am looking forward to your next test.  Denice

Comment by George Lewter on March 3, 2014 at 8:02pm

The White Crawl Glaze on my conical bottle consists of:

Nepheline Syenite 70

Magnesium Carbonate 25

Ball Clay (OM4) 5

This glaze over licorice was a really good match with both glazes well melted and largely leveled out, while retaining distinct borders, and not moving too much.

The White Crawl needs to go on thick enough that a network of cracks forms over its surface as the water is pulled out of it. It will then be prone to flaking off the base glaze during handling and even in the firing, particularly if it is applied over a powdery, poorly bonded base glaze. I want to try this glaze over C Harris Tenmoku next.

Thanks to Eric Evans at MIY Ceramics for sharing the recipe with us.


Stars
Comment by Norm Stuart on March 2, 2014 at 1:24pm

Magnesium crawl glazes have high surface tension, but this can be sabotaged by additional flux from the underlying glaze.

This is a crawl glaze made from a glaze with 30% Magnesium Carbonate over a stiff glaze on the left, and over a more fluid high-flux glaze on the right.

Cone 6 Oil Spot glazes create high surface tension through with a different ingredient, 10% or more of refractory colorants like Zircopax and or Mason Stains.   These glazes are more resistant to mixing with flux from the underlying glaze.

So the more fluxed and fluid glaze on the right is preferable to break the refractory over-glaze into smaller fragments.


Stars
Comment by juli long on March 2, 2014 at 12:24pm

looks like a bunch of alien faces!!! Too cool!

Comment by George Lewter on March 2, 2014 at 8:51am

The white crawl glaze is a studio glaze at MIY Ceramics in Hollywood FLA. Erik Evans could give us the recipe, or I can get it when I'm there next. Erik is now a member of the Insight-Live Users Group, and will be adding recipes there as he learns to use the system.


Stars
Comment by Denice E. Demuth on March 2, 2014 at 5:47am

George do you make your own White Crawl glaze or is it purchased?  I like the edge on the bottom, it catches the excess glaze and makes it look like the pot is growing out of the ring of glaze.    Denice

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service