Forum Discussions (387)

Discussions Replies Latest Activity

Glaze recipes using Alberta Slip

I have been looking at some glaze recipes that use Alberta Slip.  I found the recipes at Albertaslip.com.  I also found some at the Plainsm…

Started by Chantay Poulsen in Glazes - Testing and Reporting

2 Jun 20, 2015
Reply by Chantay Poulsen

under fired top shelf pyro cones

My c5 cones, too shelf only does not fire to maturity. The below shelves all fire to maturity. I plug top peep at 1000degrees and turn off…

Started by Billie in Firing Techniques

1 Jun 19, 2015
Reply by Norm Stuart

Overfiring

Does anyone have experience with their kilns over firing? It seems that most struggle with under firing.

Started by Shelley Bauer, Blue Apple Studio in Firing Techniques

1 Jun 19, 2015
Reply by Norm Stuart

Stars

Recipe of Reliable matt (very) yellow cone 6 glaze

Does anyone have a reliable recipe of a Matt yellow (strong yellow)cone 6 glaze? I'm starting to make my own glazes and my attempts with a…

Started by Danielle Gouvea Costa Resende in Glazes - Recipe Exchange

25 Jun 16, 2015
Reply by Harold Roberts

Stars

Post firing/glazing repairs

I have made a vessel sink for a guest bathroom. With this design there is no need for holes for the faucet and handles, the only plumbing a…

Started by Marla Stroup in Altering and Decorating Forms

7 Jun 11, 2015
Reply by Marla Stroup

Any recommendations for a potter's wheel?

Okay Ladies and Gents,  I've been at a school of the arts for almost 3 years and have been using their equipment in exchange for teaching c…

Started by Cyndy Littleton in Pottery Equipment

5 Jun 4, 2015
Reply by George Lewter

Dry glaze application

Hello! I read a post about dry glaze application. I cannot find it now, but wanted to ask how do you apply these dry glazes, for example to…

Started by luis goldfarb in Glazes - Application Techniques

3 Jun 3, 2015
Reply by Norm Stuart

Want to spray unsieved glazes?

If you want to have speckled glazes where the specks are generated by particles in the glaze, you should not ball mill or sieve the glaze.W…

Started by Daniel Spruyt in Glazes - Application Techniques

5 Jun 3, 2015
Reply by Daniel Spruyt

Stars

Dry Glazes, Slips, Terra Sigilatta and Engobes for Cone 6 - Recipes and Techniques

Note 8/32/2014 from George Lewter - added the words "Slips" and "Terra Sigilatta" to make this topic more inclusive of the non-melted mater…

Started by Jan Wallace in Glazes - Recipe Exchange

17 Jun 2, 2015
Reply by Norm Stuart

Stars

Assad Black

Has anyone tried out Assad Black from John Britt's Mid-Range Glazes? There is a photo of one of Christa Assad's pieces on page 140 and the…

Started by Gina Skillings in Glazes - Development and Adjustment

12 Jun 1, 2015
Reply by Gina Skillings

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014