If you want to have speckled glazes where the specks are generated by particles in the glaze, you should not ball mill or sieve the glaze.
What if you want to spray these glazes anyway? The conventional spray gun will be clogged quickly!
Solution: the good old vaporizer !
Two tubes of about 1/4” at a right angle and compressed air of about 50-60 psi will do (you can even use your lungs! but you need a lot breath!)
I had an old pistol for inflating tires where the manometer was broken.
Indeed it still can be used. The attached pictures are self explanatory.
The tubes used cannot be clogged and the spray is excellent. See also the attached picture of a pot sprayed with a glaze containing rather coarse iron particles.

Views: 416

▶ Reply to This

Replies to This Discussion

Wow ... thanks, exactly the information I was looking to find!

Hello! This is exactly what I was looking for! many thanks for this info. I'd like to ask if it was possible to attach a recipient for the glaze so you can move the spray gun freely. Could a small plastic base be attached to it? Thank you!!!



luis goldfarb said:

Hello! This is exactly what I was looking for! many thanks for this info. I'd like to ask if it was possible to attach a recipient for the glaze so you can move the spray gun freely. Could a small plastic base be attached to it? Thank you!!!

Yes, obviously this is more handy. I must say that this kind of adaptation is still in my mind, but so far I didn't make it. With some simple DIY skills you can use e.g. an empty jam jar, pierce the lid and with some simple plumbing accessories fix the gun on the lid.

Thanks Daniel. I wonder if this could also work for higher density glazes with iron filings, etc. I think glazes should have less water content so that the iron filings don't sink to the bottom. (Please excuse my English :-))



luis goldfarb said:

Thanks Daniel. I wonder if this could also work for higher density glazes with iron filings, etc. I think glazes should have less water content so that the iron filings don't sink to the bottom. (Please excuse my English :-))

Hi, your English is as good as mine, it is also not my native language (Dutch or French)

The times I used my system, it was with relatively fine Iron filings. My glazes are often quite liquid (90 ml water for 100g dry glaze) and this works fine with the device. Of course, the stem of the device should not be too long ( not more than 10 cm I guess) and from time to time stir or shake the glaze recipient.

Good luck.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service