I have been looking at some glaze recipes that use Alberta Slip.  I found the recipes at Albertaslip.com.  I also found some at the Plainsman clay website.  Some of the recipes are on the Digital Fire under glazes on the main menu page.  I have not been able to find any of them on Insight Live.  I am wondering why this is.  I like using Insight Live to calculate my glaze batches.  I am slowly learning about glaze chemistry.  Is it possible that the glazes are there and I am entering the name wrong?  If anyone has information on this please let me know. Thanks.

Some of the glazes I am planning to try out are:

Alberta Slip Rutile Blue

Alberta slip cone 6 Black

Alberta slip Glossy Brown

Alberta slip Glossy Base.

Views: 551

▶ Reply to This

Replies to This Discussion

Chantay - Please feel free to enter any recipes you like into our Insight-Live database.

Although Insight-Live is managed by Digitalfire, this doesn't mean all glaze recipes found on Digitalfire webpages are already in our database.  The raw material Alberta Slip is already one of the hundreds of raw materials available to choose from, with the chemistry managed by Digitalfire.

Thanks for information Norm.  I was just surprised that the glazes were not already in the database.  I will add them as I go along.  Just loaded a bisque with about 200 test tiles.  I don't like the glazeing part, but I am determined to make some progress. 

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service