I'm trying to refine my skills at slip trailing and struggling. I'm having trouble getting slip to squirt in a smooth flowing manner, sometimes on top of one another and with feathering.

Mixing it thin and putting lots of Epson salts in it to flocculate helps a great deal but I can't get it to flow like I see in these two videos.

https://www.youtube.com/watch?v=NJOYTqST5b8

https://www.youtube.com/watch?v=_PyKDYCNzF4

 

Do you have any suggestions?

Are there some additives that would improve the flow?

Views: 475

Reply to This

Replies to This Discussion

When I have done any wet slip work like feathering or marbling, I havent added anything to slip - just clay, water and some oxides for colour. I suppose results maybe depend on clay body a little. Are you decorating freshly thrown or leather hard pots?
I've found runny slip techniques much easier on freshly thrown pots.

Maybe I am too quick to add additives. I will give it a try your way.

Thanks for the suggestion

 I found my  solution in small tattoo bottles that I bought  on eBay for $.75 a set. They work like magic. I'm actually doing glaze trailing on bisque.Glaze trailng on bisque actually works very well.  If you screw up, wash it off and try again.

16pc-Set-Henna-Kit-Applicator-Nozzles-Bottles-Paste-Tattoo-Body-Art-Drawing-Tool

What a great discovery. I could not find them at first, but then discovered similar bottles for henna art. Can't wait for them to arrive (it will be a while, because they are from China).

Lawrence Weathers said:

 I found my  solution in small tattoo bottles that I bought  on eBay for $.75 a set. They work like magic. I'm actually doing glaze trailing on bisque.Glaze trailng on bisque actually works very well.  If you screw up, wash it off and try again.

16pc-Set-Henna-Kit-Applicator-Nozzles-Bottles-Paste-Tattoo-Body-Art-Drawing-Tool

Larry:

Got shut down at work today, 1/2" of ice will do that. Gave me the chance to watch your videos, a little chemistry at work. The base has gum in it; giving it just a slightly thicker viscosity, and structure (resist running). The decorating slip I suspect is sodium based; if you noticed the base slip "seemed" to repel it. Interesting to watch the reaction ( which you call running).

Could be possible the base has gum and sodium based; and the decorating slip is then repelled.

Tom

Right now I am frozen out of my studio. When it warms up a bit I would check the slip recipe to see if it is sodium based. However my little bottles seem to have solved the problem quite nicely. Thanks for your suggestions.

I do a bit of glaze trailing with my work. The bottle/tip is designed for oiling small model trains. The price was very reasonable and the supplier was on Ebay and located in the US, but I have since lost the address/contact. Tips are metal and rather long which seemed easier to use than the short ones (more like drawing with a pen/pencil) If you should come across them give me a shout. thanks. carl

Get into the Way-Back machine, and take a look at Charan Sachar's video posted in 2009. Using miniature cake decorating funnels, home made from mylar, he achieves a level of sensitivity and control that is impossible when squeezing a thick plastic bottle or syringe. 

Thanks george

That is a technique that I will have to try

Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Your final price could be less or more - things change.

American Weigh Black Blade Digital Scale, 1000g X 0.1g $11.08 

For the non-digitally inclined the old standard Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2021   Created by George Lewter.   Powered by

Badges  |  Report an Issue  |  Terms of Service