Lawrence Weathers's Discussions (119)

Discussions Replied To (74) Replies Latest Activity

"Wow, thanks for all the research. Did you ever think about writing all this up as an…"

Lawrence Weathers replied Aug 22, 2018 to How to do Acrylic paint pouring with ^6 glaze ??

7 Aug 22, 2018
Reply by Norm Stuart

"How is this different from sodium silicate?"

Lawrence Weathers replied Aug 21, 2018 to How to do Acrylic paint pouring with ^6 glaze ??

7 Aug 22, 2018
Reply by Norm Stuart

"I'm experimenting with a variety of additive's such as Sodium silicate, Epsom salts,…"

Lawrence Weathers replied Aug 20, 2018 to How to do Acrylic paint pouring with ^6 glaze ??

7 Aug 22, 2018
Reply by Norm Stuart

"Thanks george That is a technique that I will have to try"

Lawrence Weathers replied Jan 24, 2017 to Slip trailing

9 Jan 24, 2017
Reply by Lawrence Weathers

"Right now I am frozen out of my studio. When it warms up a bit I would check the sli…"

Lawrence Weathers replied Jan 15, 2017 to Slip trailing

9 Jan 24, 2017
Reply by Lawrence Weathers

"What end up working best is mixing a little Elmers with the Glaze.  If you put too m…"

Lawrence Weathers replied Jan 12, 2017 to glaze flaking off in high magnesium glazes

6 Jan 12, 2017
Reply by Tom Anderson

" I found my  solution in small tattoo bottles that I bought  on eBay for $.75 a set.…"

Lawrence Weathers replied Jan 12, 2017 to Slip trailing

9 Jan 24, 2017
Reply by Lawrence Weathers

"tom That gives me a good starting point thanks Larry"

Lawrence Weathers replied Oct 24, 2016 to glaze flaking off in high magnesium glazes

6 Jan 12, 2017
Reply by Tom Anderson

"hi Tom Thanks for the suggestions I think I will try both approaches. You have any…"

Lawrence Weathers replied Oct 24, 2016 to glaze flaking off in high magnesium glazes

6 Jan 12, 2017
Reply by Tom Anderson

"Maybe I am too quick to add additives. I will give it a try your way. Thanks for the…"

Lawrence Weathers replied Oct 18, 2016 to Slip trailing

9 Jan 24, 2017
Reply by Lawrence Weathers

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service