"Catherine - 999 is simple, but probably not what you want to choose for a heating ra…"

Norm Stuart replied Jun 29, 2017 to Am I dense or what

2 Jun 30, 2017
Reply by catherine simmons

"Kathryn - All of the recipes for the glazes I use are available on George Lewter's I…"

Norm Stuart replied Jun 28, 2017 to Slow Cooling

13 Jun 28, 2017
Reply by Norm Stuart

"All you would add to the Tween-80 is a colorant like black mason stain, iron oxide,…"

Norm Stuart replied Jun 17, 2017 to Mocha Diffusoin

18 Aug 17
Reply by tony remington

"Interesting. That 10% loss of weight would probably be quite different with a differ…"

Norm Stuart replied May 25, 2017 to Leather hard to glaze fired weight difference

4 May 25, 2017
Reply by Norm Stuart

"Hi Tom - 100 grams of wet clay should weigh about 52 to 57 grams after it's bisqued…"

Norm Stuart replied Apr 22, 2017 to Leather hard to glaze fired weight difference

4 May 25, 2017
Reply by Norm Stuart

"Arva - Unfortunately the percentage of Mason Stain you need to use varies by the col…"

Norm Stuart replied Apr 4, 2017 to Help with Mason Stain 6021

3 Apr 4, 2017
Reply by Norm Stuart

"Yes that's the difference between light and dark rutile. But which ever you purchase…"

Norm Stuart replied Jan 22, 2017 to Light Rutile Substitute

11 Mar 7, 2017
Reply by Judith Stoudmann

"We have three different bags of rutile and each one looks different. One produces a…"

Norm Stuart replied Jan 10, 2017 to Light Rutile Substitute

11 Mar 7, 2017
Reply by Judith Stoudmann

"That's a really nice result. Trial and error layering glazes can produce phenomenal…"

Norm Stuart replied Jan 2, 2017 to Soda firing

8 Jan 2, 2017
Reply by Norm Stuart

"Robin - Nepheline Syenite is a notorious source of free sodium and potassium ions wh…"

Norm Stuart replied Dec 8, 2016 to Specific Gravity and Bentonite

4 Dec 10, 2016
Reply by Robin Cherfane

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service