I'm having difficulty understanding cooling segments. How can a kiln cool at 999degrees per hour (1900 from 2115)when it seems to take forever to go from 400 to 200. It seems it would need an AC unit to kick in to achieve that fast of a temp drop
By the way I have a used L&L

Views: 266

▶ Reply to This

Replies to This Discussion

Catherine - 999 is simple, but probably not what you want to choose for a heating ramp because it could shorten the life of the elements in some kilns which don't have a protective over-ride to avoid excess heating element temperature. But it's a convenient programming notation for cooling ramps.

When you specify a 999 ramp during a heating or cooling ramp, the actual rate achieved is obviously going to be quite different to what you specified. It simple means heat as fast as possible or cooling without added heat.

Our kiln is relatively overpowered relative to its size, so a 999 ramp is actually a 999 ramp until it heats up to about 1,600 F when it starts to slow down to a real ramp of about 670 per hour, and above 2,000 F it's slower still.  Our empty kiln could complete a Cone 6 firing within about 2 hours and 40 minutes. With ware in the kiln it would probably take a little longer, but it would still heat up quick enough to crack and break much of the ware in the kiln.

We use auto-fire pre-programmed firings in our kiln controller.  See page 24 of the Bartlett Genesis Kiln Controller to see the firing profiles Bartlett uses in their kiln controllers.  PDF file here -- Genesis Kiln Controller - (see page 24)

Slow-cools are added onto the firing with additional buttons like a microwave oven. A nice toy to add to a kiln for $329 Bartlett Genesis Controller  or you can buy their earlier V6-CF model for $219.

Bartlett Genesis kiln controller

Bartlett V6-CF kiln controller

.

.

The older RTC-1000

requires you to program each firing every time, yet costs $219 just like the more capable V6-CF

Thank you for your response. I really appreciate your time and input to this forum

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service