Kabe Burleson's Discussions (55)

Discussions Replied To (38) Replies Latest Activity

"They make a device, I do not know what they are called, that one can use to lift a p…"

Kabe Burleson replied Jun 21, 2014 to Throwing questions

14 Jul 6, 2014
Reply by Leo Villaroman

"Hi Dani. Glazing can be a challenge. Record keeping by the motto " I'll remember and…"

Kabe Burleson replied Jun 11, 2014 to Glaze Development for Dummies

13 Jun 11, 2014
Reply by Norm Stuart

"I spray most things three slow coats and I do not know what the thickness would be. …"

Kabe Burleson replied Apr 13, 2014 to how thick should your glaze be sprayed on and how do you tell if it is that thick?

13 Apr 14, 2014
Reply by Jennifer Arthur

"Hi Nancy. I do not know if this will work or not. What you want is large  brown spot…"

Kabe Burleson replied Dec 27, 2012 to How to create light brown specks in low fire glaze

8 Jun 18, 2013
Reply by Nancy Krug

"I don't know if this will help or not. I have a handout from college "Guide to use o…"

Kabe Burleson replied Dec 26, 2012 to How to create light brown specks in low fire glaze

8 Jun 18, 2013
Reply by Nancy Krug

"Well that's a bummer Donna. I have never used stilts so I do not know the preperatio…"

Kabe Burleson replied Dec 23, 2012 to warping platters

2 Dec 23, 2012
Reply by Donna Ferrara

"Hi Carl. I have a cone 10 recipe for a "Metallic Black Slip" If you add the colorant…"

Kabe Burleson replied Dec 21, 2012 to Need some engobe help please.

5 Dec 21, 2012
Reply by Kabe Burleson

"Hey Leigh, If you try these two clear glazes and they do fit, please let me know and…"

Kabe Burleson replied Dec 8, 2012 to Looking for a good clear glaze for little loafers

5 Dec 16, 2012
Reply by Leigh Whitaker

"I mix my own clay so I do not know if this will fit Little  Loafers.  You could test…"

Kabe Burleson replied Dec 5, 2012 to Looking for a good clear glaze for little loafers

5 Dec 16, 2012
Reply by Leigh Whitaker

"I am still in the learning stage of glaze chemistry So the stuff I do not know out w…"

Kabe Burleson replied Nov 26, 2012 to Wollastonite and Whiting

2 Dec 10, 2012
Reply by Sharon Canfield

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014