Hi All

I fired a student's oval platter (cone 6) on triangular stilts.  It warped, I think because I placed the stilts incorrectly. I was thinking of refiring it with out the stilts.  Has anyone had experience refiring something like this?  will it flatten out?

Views: 202

▶ Reply to This

Replies to This Discussion

Well that's a bummer Donna. I have never used stilts so I do not know the preperation involved when someone is glazing. My first concern would be if the foot was glazed or not and if it was to be refired would it stick to the shelf. As far as it flatting back out seems like it might. I think I would pray, light incense, chant a mantra, sacrifice a fat chicken and maybe even face Mecca first, just to be on the safe side and to make sure I had all the bases covered.  It may depend on the memory of the clay. Tiles don't lay down if they are warped but often that has to do with how they were handled before the firing, not because of the firing. Good luck, Merry Christmas, and Happy firing.

thanks for your thoughts!  I think it might flatten out some too....the bottom was glaze free, but my student (12 yr old) decided to take it home...I gave her a few old posts to prop it with , and if she likes the way it looks, she'll glue them to the bottom for legs....it's hard to know how much the piece was manipulated during the making...another girl's came out perfectly

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service