What Are the Best White Stoneware and Porcelain Bodies for Single Firing with the SH palette?

I have been using Laguna B-mix5 since 2009 with minimal problems. My Michigan supplier appears to have ceased operations. Does anyone know what body Steven is currently using after attending one of his 2013 workshops. I heard at one point he had switched to a Standard porcelain or 182 which is listed as:

182 WHITE STONEWARE BODY (Cone 6-10)

Near white plastic stoneware body. Good for use with bright glazes. Available with and without fine grog. 
Shrinkage:  11% at C/8, 12% at C/10.
Absorption:  3% at C/8, 2.1% at C/10. 

As you can see this clay is at the bottom of its range at cone 6 and has high absorption even at cone 8, so I'm thinking it might not be a terrific cone 6 body.

I would use one of the Standard Ceramic Supply bodies if possible, as there is a distributor within 50 miles of me. We also have Runyan which is a local manufacturer with a very sophisticated clay compounding facility. But they don't seem to have knowledge of what constitutes a good single firing body.

Views: 313

Replies to This Discussion

I emailed Stephen Hill and he told me he uses Coleman Cone 10 porcelain, yes Cone 10 with his Cone 6 firing schedule.

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service