Tom Waggle's Discussions (16)

Discussions Replied To (11) Replies Latest Activity

"If nobody has tried the SH Red Orange by itself as a liner it is gorgeous and has a…"

Tom Waggle replied Dec 2, 2013 to Pinholes and craters

22 Oct 17, 2016
Reply by Tom Anderson

"I still need to make a set of test tiles, actually throw some test cylinders so I ca…"

Tom Waggle replied Dec 2, 2013 to Pinholes and craters

22 Oct 17, 2016
Reply by Tom Anderson

"I asked Stephen Hill which of his glazes are suitable for liner glaze and he told me…"

Tom Waggle replied Dec 2, 2013 to Pinholes and craters

22 Oct 17, 2016
Reply by Tom Anderson

"talked to my kiln distributor today.  He asked if the Envirovent on my Skutt was wor…"

Tom Waggle replied Dec 2, 2013 to Pinholes and craters

22 Oct 17, 2016
Reply by Tom Anderson

"For the record: The clay body I am using is LAGUNA 607 Cone 6 Buff Stoneware. It is…"

Tom Waggle replied Dec 2, 2013 to Pinholes and craters

22 Oct 17, 2016
Reply by Tom Anderson

"Thanks for your reply. I slow down my BISQUE firing on its way UP, the range when th…"

Tom Waggle replied Dec 1, 2013 to Pinholes and craters

22 Oct 17, 2016
Reply by Tom Anderson

"I emailed Stephen Hill and he told me he uses Coleman Cone 10 porcelain, yes Cone 10…"

Tom Waggle replied Dec 1, 2013 to What Are the Best White Stoneware and Porcelain Bodies for Single Firing with the SH palette?

1 Dec 1, 2013
Reply by Tom Waggle

"I cannot explain how or why some of my pieces come out with no defects and others do…"

Tom Waggle replied Dec 1, 2013 to Pinholes and craters

22 Oct 17, 2016
Reply by Tom Anderson

"If anyone is using cone 6 stoneware successfully without pinholes and craters could…"

Tom Waggle replied Dec 1, 2013 to Pinholes and craters

22 Oct 17, 2016
Reply by Tom Anderson

"I think it is important to stress the hold at Cone 5, it will fall between 30 and 60…"

Tom Waggle replied Mar 20, 2013 to Cone 6 firing schedule for SCM etc glazes

23 Jun 27, 2013
Reply by Norm Stuart

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service