Hi,
My name is Maria and a somewhat amateur at pottery
This is my first post and I'm so glad to have found this forum!
I have a kiln and bought a potter's wheel of Shimpo RK-3E.
Watched a video on YouTube where the craftsman made ​​a slip. I was delighted.
He works on the wheel and with the raw clay begins to decorate with a liquid using Slip Trailer Applications.
Does someone could help me, informing the liquid that is used to decorate the raw clay is Engobes or underglaze?  
I want to buy the product and would like to really know right.
If Engobes, should I buy liquid or powder?
And Underglaze can use the raw clay?

Can I post a link to the video?

You can see and give a better answer.

I thank those who help me  
Thank you

Views: 450

▶ Reply to This

Replies to This Discussion

Maria,

You can quickly make slip using using dried scrap of your clay body.

Just weigh the scrap then add it to water in an old blender. See attached.

You can make trailing slip or brushing slip, or dipping slip just by controlling the amount of water.

If you want colored slip you can buy Mason stain colors from any dealer.  If you clay body is white usually add color 10% by weight of your dry scrap will work .  Here is link to Mason colors.

http://www.masoncolor.com/ceramic_stains.asp

This forum is nearly dead.  You can get more help and easier to use on ClayArt Daily.  Here is link:

http://ceramicartsdaily.org/community/forum/23-clay-and-glaze-techn...

See you there.

John255


John Forstall said:

Maria,

Você pode rapidamente fazer deslizar usando usando sucata seca do seu corpo de barro.

Apenas pesar a sucata, em seguida, adicioná-lo à água em um liquidificador velho. Veja em anexo.

Você pode fazer de fuga deslizamento ou escovar deslizamento, ou mergulhando deslizamento apenas por controlar a quantidade de água.

Se você quiser deslizamento de cor você pode comprar pedreiro cores mancha de qualquer revendedor. Se você corpo de barro é branco geralmente adicionar cor 10% em peso de seu recado seco vai funcionar. Aqui está o link para as cores Mason.

http://www.masoncolor.com/ceramic_stains.asp

Este fórum é quase morto. Você pode obter mais ajuda e mais fácil de usar em ClayArt Daily. Aqui está o link:

http://ceramicartsdaily.org/community/forum/23-clay-and-glaze-techn ...

Vemo-nos lá.

John255

Hi John255

Thanks for your help.
I live in Portugal and I buy stuff in the U.S. or UK.

I am a member of the forum ceramicartsdaily and has asked for help.
You can see what I posted here:
http://ceramicartsdaily.org/community/topic/4511-amateur-needing-help

Also will be able to see the video with the problem I want to know. This slip of the video is done with engobe or underglaze?
Bought slip (engobe) color powder. How much should I add water to 100g?

See there and read my topic

You typically need to add about 2% to 10% color to a clay to color an englobe.

I've found that adding "Pat Horsely's Score No More" to your clay body helps the slip adhere.

Pat Horesely's Score No More

100.0%   Dry Clay - the type you're using
2.0%   Feldspar Custer Potash
2.0%   Bentonite
2.0%   Gum Arabic or Xanthan Gum
0.5%   Darvan

Hi Norm Stuart

Thanks for your help.

I bought the powder already in engobe colors.
Can you tell when I put water in engobe powder, I add water along with some substance to stick with engobe glazed effects?



Norm Stuart said:

You typically need to add about 2% to 10% color to a clay to color an englobe.

I've found that adding "Pat Horsely's Score No More" to your clay body helps the slip adhere.

Pat Horesely's Score No More

100.0%   Dry Clay - the type you're using
2.0%   Feldspar Custer Potash
2.0%   Bentonite
2.0%   Gum Arabic or Xanthan Gum
0.5%   Darvan

If you actually purchased a dry pre-mixed englobe, such as this product:

http://www.amaco.com/shop/product-463-engobes-se-lead-free.html

You simply add water until it is like thick cream, as the product instructions say.

If you purchased a color to add to an englobe, you need to mix it with the clay you are using or an englobe recipe. This article contains a typical englobe recipe.

http://ceramicartsdaily.org/ceramic-supplies/ceramic-raw-materials/...

Bought a covering premixed dry.
Can anyone tell me if when I put water in engobe powder, I add with the water some substance to stick with engobe glazed effects? glycerin, olive oil .... ?
I'll slide the engobe in various colors using the Slip Trailers.
I want the colors do not mix.



Norm Stuart said:

Se você realmente comprou um englobe pré-misturado seco, como este produto:

http://www.amaco.com/shop/product-463-engobes-se-lead-free.html

Basta adicionar água até que fique como um creme espesso, como dizem as instruções do produto.

Se você adquiriu uma cor para adicionar a um englobe, é preciso misturá-lo com o barro que você está usando ou uma receita englobe. Este artigo contém uma receita englobe típico.

http://ceramicartsdaily.org/ceramic-supplies/ceramic-raw-materials/ ...

The pre-mix should have everything it needs, so just add water. You can add a thickener, a very plastic clay called bentonite, but your pre-mix should already have it included.

Just let each color of englobe dry fully before adding the next, and they won't mix.

Maria Correia said:

Bought a covering premixed dry.
Can anyone tell me if when I put water in engobe powder, I add with the water some substance to stick with engobe glazed effects? glycerin, olive oil .... ?
I'll slide the engobe in various colors using the Slip Trailers.
I want the colors do not mix.



Norm Stuart said:

Se você realmente comprou um englobe pré-misturado seco, como este produto:

http://www.amaco.com/shop/product-463-engobes-se-lead-free.html

Basta adicionar água até que fique como um creme espesso, como dizem as instruções do produto.

Se você adquiriu uma cor para adicionar a um englobe, é preciso misturá-lo com o barro que você está usando ou uma receita englobe. Este artigo contém uma receita englobe típico.

http://ceramicartsdaily.org/ceramic-supplies/ceramic-raw-materials/ ...

Message sent to you with the link of the video in question.
Could you help me?
I await contact


Norm Stuart said:

The pre-mix should have everything it needs, so just add water. You can add a thickener, a very plastic clay called bentonite, but your pre-mix should already have it included.

Just let each color of englobe dry fully before adding the next, and they won't mix.

Maria Correia said:

Bought a covering premixed dry.
Can anyone tell me if when I put water in engobe powder, I add with the water some substance to stick with engobe glazed effects? glycerin, olive oil .... ?
I'll slide the engobe in various colors using the Slip Trailers.
I want the colors do not mix.



Norm Stuart said:

Se você realmente comprou um englobe pré-misturado seco, como este produto:

http://www.amaco.com/shop/product-463-engobes-se-lead-free.html

Basta adicionar água até que fique como um creme espesso, como dizem as instruções do produto.

Se você adquiriu uma cor para adicionar a um englobe, é preciso misturá-lo com o barro que você está usando ou uma receita englobe. Este artigo contém uma receita englobe típico.

http://ceramicartsdaily.org/ceramic-supplies/ceramic-raw-materials/ ...

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014