I need to change my white glaze to one that will withstand the test of time.

I see the one I have used for 30 years is checking. Please let me know if you have a great replacement.

Views: 1467

▶ Reply to This

Replies to This Discussion

What about the cone 6 faux-majolica recipe in  Mastering Cone 6 Glazes? Haven't tested or used it myself, but it looks great in the book on porcelain.

Thanks George,

I have the book so I will look it up.

I like to know where the glazes come from .

That sound like a good start. 

With so many to look at I didn't know where to begin.

I will test it with my other glazes.

I would use the white satin before the majolica for dinner ware if you are going to take the recipe from Mastering Cone 6.  I think it is the Glossy 1 with 5% tin oxide.  It is a stable glaze and I believe it is the recipe for the liner glaze (minus the tin).  You could also take the recipe Ron Roy's Black from frogpondpottery - remove the colorants and add tin.  It is a liner glaze.  If you would like it to be a little warmer add rutile.  Up to 6% would be nice and increase the stability.

George Lewter said:

What about the cone 6 faux-majolica recipe in  Mastering Cone 6 Glazes? Haven't tested or used it myself, but it looks great in the book on porcelain.

Thanks Donna..... I will test the white satin as well.  These are good leads which I appreciate.

I use the majolica white from Mastering Cone 6 Glazes adding 12% zircopax.  It is not quite as glossy as the glossy base although it will take a clear gloss over it very well. I get many compliments on this white.

I have also used the glossy base 1 white.  I do not have access to the G-200 that the book recommends so had to go with Custer Feldspar or Minspar with the formula adjusted for low K Custer Feldspar and Texas talc.  Alternately, have mixed it with Minspar and gotten similar results using zircopax. I received updated recipes from Ron Roy to account for the reduced K2O that is currently coming out of the Custer Feldspar mine.He is reachable on the clayart message board.

Ron Roy's black is the Glossy Base 2 from Mastering Cone 6 - you'll need to adjust the Feldspar on it as well, the recipes on FrogPond for the black don't take into account the low K2O currently being shipped by the mine.

Basically you need to alter Black#3 var 1 by increasing the Custer Feldspar by 4% and reducing the silica by 3.5% and the EPK by 0.5%.  Ron gave me these adjustments and the black is EXCELLENT.  It also makes a nice white if you eliminate the colorants and add zircopax (I use spectralux).  Fire to cone 6, drop to 1900 then control your cooling down to 1400 @125/hour.

Brent, Thanks for your valued info. I do appreciate it. 

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service