Hi- does anybody have Emmanuel Cooper's recipe "WSG31 Clear"? I read that this is recommended by the Mason Co. for mixing with their stains. Thanks. Joan C.

NOTE: Replies are posted from oldest to newest, so the most recent posts will be at the bottom of the last page.

Views: 395

▶ Reply to This

Replies to This Discussion

Hang in there Joan.

I'd like to see you get a response on this one.

John255

Joan,

I could not get an email response from Mason Colors stain company so I called them.  They recommend the following formula for transparent large cone 6.

F-38 frit          32

Kona F-4 Spar  26

Silica              19

Whiting           13

EPK                10

The formula looks quite old.  F-38 is and odd frit by Fusion Co. that contains about 18% strontium carbonate.  The closest Ferro frit is 3292, but it only has 4% strontium.   I personally don't think that small amount of strontium is going to influence the colors very much.

For the other components of F-38 the Ferro frit 3124 is fairly close, but it does not contain strontium.  When I get around to testing this formula on stains I will use frit 3124 and for one batch add about 10% strontium carbonate to see if it indeed affects the colors significantly.

Regards,

John255

 

Wow! Thank you John! I'm not quite sure how to reply on this site- think I just managed to repost your post somehow. If you do get around to testing for colour response, please post pics of your results, and I will do likewise- Joan C. 

Has anyone tried Emanuel Cooper's Shocking Pink at cone 6, or tried fluxing it down?

I understand he was well-known for developing this method of pink with barium, zinc and nickel.

40.0%   Barium Carbonate
35.0%   Potash feldspar
15.0%   Zinc oxide
5.0%   China Clay
5.0%   Silica
2.4%   Nickel Carbonate

Joan,

Your post made it OK.

I too find the site a bit hard too get used to.

I also posted your subject over on Clayarts Daily where there is a bit more traffic.

http://ceramicartsdaily.org/community/topic/3987-clear-6-for-mason-...

Norm,

That looks interesting, but I stay away from Barium because I want to get as many retirement checks as possible.

John255

You can always replace Strontium Carbonate for Barium Carbonate without changing the color much.

John Forstall said:

Norm,

That looks interesting, but I stay away from Barium because I want to get as many retirement checks as possible.

John255

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service