Donna Ferrara's Discussions (16)

Discussions Replied To (14) Replies Latest Activity

Stars

"thanks for your thoughts!  I think it might flatten out some too....the bottom was g…"

Donna Ferrara replied Dec 23, 2012 to warping platters

2 Dec 23, 2012
Reply by Donna Ferrara

"i'm not sure it's a wrong or right issue, just make sure the fit is good because you…"

Donna Ferrara replied Jul 18, 2012 to Bisque at Cone 10 and then Glaze at Cone 6

32 Apr 26, 2013
Reply by Norm Stuart

"then it's all good ; )"

Donna Ferrara replied Jul 18, 2012 to Bisque at Cone 10 and then Glaze at Cone 6

32 Apr 26, 2013
Reply by Norm Stuart

"hi Shine in reading this discussion, my largest concern would be the fit between the…"

Donna Ferrara replied Jul 17, 2012 to Bisque at Cone 10 and then Glaze at Cone 6

32 Apr 26, 2013
Reply by Norm Stuart

Stars

"very true, Patricia. I have also sprayed the piece lightly with hair spray and then…"

Donna Ferrara replied Jun 14, 2012 to Glaze Tips & Tricks

18 Jul 21, 2016
Reply by Vladimir

"thank you! I was slow in getting started here, largely due to lack of computer skill…"

Donna Ferrara replied May 30, 2012 to Supporting Membership Strengthens and Enhances the C6P network

23 Jul 1, 2012
Reply by George Lewter

Stars

"thanks for posting- great combinations and comments about the glazes  iHave a questi…"

Donna Ferrara replied May 5, 2012 to Glaze Tests

32 Jul 1, 2017
Reply by Sofia Donovan

"http://digitalfire.com/4sight/material/bentonite_106.html I found this really inter…"

Donna Ferrara replied Apr 15, 2012 to Bentonite Anyone?

10 Jun 25, 2013
Reply by Angela Davis

Stars

"you could break your mug and see if thebumps are in the clay bod or on top"

Donna Ferrara replied Apr 10, 2012 to Help! Blisters or Pinholing

8 May 31, 2012
Reply by lessie hostilo

Stars

"hi can you crush the bumps and they break?  when you said raised bumps, I wondered i…"

Donna Ferrara replied Apr 10, 2012 to Help! Blisters or Pinholing

8 May 31, 2012
Reply by lessie hostilo

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service