Hope this is the correct way to ask a question.  How do you get a clean line between 2 colors on the rim of a mug?  Such as a liner glaze inside and a different one on the outside.  I have noticed pictures on the site with a very clean break between the glazes just at the top of the rim.   

Views: 1345

▶ Reply to This

Replies to This Discussion

Hi Bill,
I am not a really experienced glazer so if I wanted to accomplish that I would brush it on or spray it on. If I attempted to dip that it would be a disaster! ;)

I do not get a sharply precise line with my approach as there is normally a very slight overlap of the two glazes, but... I glaze the inside with my liner glaze and after pouring it out of the piece, touch the edge of the lip in the glaze.  After it has dried, I press the piece, right side up into the bucket of glaze and allow the glaze to come up the outside to hit the liner glaze.  I have also waxed the rim after doing the inside liner and allowing it to dry and then followed the same process as above to get a sharper line where the two glazes meet, as the wax prevent any overlap.  Hope this makes sense.  -carl

Thanks Jennifer & Carl.  Still working with it.  Got some ideas from a Google search to try also.

part of the trick is using glaze that doesn't move much.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service