I was surfing the internet and came across a foreign site that had a wood fired raku kiln built out of a barrel drum and it got me thinking that I could do that.  I began researching it a little bit more and it brought up some questions about the quickest and best ways of piecing it together.  I came to the conclusion that I could piece it together and rivet it together with steel rivets.  Is that feasible?  From my research steel can resist temperatures of up to 2500 degrees Fahrenheit.  Am I miscalculating things because if I'm not it seems a lot easier than using ceramic buttons or silica to seal the fire fiber to the walls of the drum.  Comments please!!

-John

Views: 668

Attachments:

▶ Reply to This

Replies to This Discussion

They make woodstoves out of sheet steel that operate with hot spots up to around 1800-1900. I think an oil drum or galvanized trash can could make a sound shell for a fiber kiln. I would still use ceramic buttons on nichrome wire to support the fiber though. Oxidizing steel in contact with ceramic fiber on the hot face might just turn into glaze.

Hi John,

In my experience steel does break down with heat work and over a short time, becomes weak, crumbles and disintegrates, hence the need to use ceramic buttons and proper kanthal wire to fasten the fibre to the side of the kiln. Kanthal wire is only a few dollars a metre and ceramic buttons are very easy to make from raku clay. Remembering that the ceramic fibre is quite thick so you need a good length of wire with each button. Here is a link to my blog with some pics of a raku kiln I built recently.

I have used a steel drum before making a gas raku kiln very similar to the design of the kiln in your attachment, but obviously as it was gas, just leave a hole in the top for a flue rather than a chimney.

http://www.janwallacepottery.blogspot.com.au/2011/06/my-new-raku-ki...

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service