Hi - I love reading these posts and now I have a question myself.  I have a Skutt kiln with an automatic control panel. I generally use the simple cone fire program and fire to cone 6 - very easy. Moving forward, I would like to experiment by firing to cone 6 and then drop the temp slowly (150 degrees/hour) to 1650 degrees and then hold for one hour - then cool normally until complete. I have read the manual 20 times and I just can't figure out how to do this. I called Skutt and the technician verbally explained it to me, but seemed a bit put off when I asked him to go through it again slowly, so I could write it down. He wouldn't go through it again, yet he agreed it's not clear in the operating guide...  Can anyone explain in detail how to do this?  Thanks  Jack

Views: 314

▶ Reply to This

Replies to This Discussion

HI Jack,

    I got this from Bartlett quite a while ago & should do the trick for you.  

You have to program user #6 first with your down ramp but you will have to set the user to have 2 segments because you will have to do a up ramp before you can do a down ramp. So basically set the first segment to a temp 2-5 degrees above the cone temp that you are firing to, then in the second segment program you down ramp. Then after that is programed go in and program your cone fire. Once that is done press (if the board is a 600 version) you will press the oF/oC select key in the upper right hand corner and then press 7,8. The screen should change to 16-S. Once this is in the screen then press the 1 key I believe it should go complete then back to idle. Then you will ado a program review and in that review it should show you 16-S. This means that the controller is programed to fire your cone fire then change over and fire your user #6. For the older kiln master skutt manuals you will want to contact skutt or check out there web site for them.

   Let me know if this works for you.  I used to do it quite a bit in my Skutt, but haven't much since I got my L&L.  Jeff

Many thanks Jeff.  I'll give it a test next week.

Jack

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service