Started this discussion. Last reply by Norm Stuart Apr 18, 2015. 9 Replies

Hi all - turning to the experts for advice. Lately I've been making large dinner plates using Standard 112 clay. I bisque at 06 and the plates come out great. Then I glaze and fire to cone 6 in my…Continue

Tags: plates

Holding at 1650 for One Hour.

Started this discussion. Last reply by Jennifer Leader Jul 7, 2012. 2 Replies

I've read a number of posts that suggest when trying to enhance "red" glazes at cone 6, it helps to cool to 1650 and then hold for one hour before proceeding. Have people found this helpful and does…Continue

How to Hold during a glaze firing

Started this discussion. Last reply by Jack Dembow May 6, 2012. 2 Replies

Hi - I love reading these posts and now I have a question myself.  I have a Skutt kiln with an automatic control panel. I generally use the simple cone fire program and fire to cone 6 - very easy.…Continue

 

Jack Dembow's Page

Profile Information

What is your experience with ceramics in general. (Long answer encouraged)
amateur
What is your current involvement with electric fired ceramics? (long answer encouraged)
amature potter, retired CEO
All our content is viewable by the public. Why do you want to be a member, when you can already see everything as a non-member?
concepts for new pots/sculptures. Interesting cone 6 glazes.
Where do you work on your ceramics projects?
home studio
How did you find this network?
Link or reference from another site

Comment Wall (1 comment)

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

At 6:12am on January 19, 2025, Ronald Morris said…

Good day,
I am RonaId Morris, I saw your profile and I decided to contact you immediately. Can you get back to me on my email (ronmorri01@gmail.com) for full details.  
Regards.

 
 
 

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service