Hi everyone! I've been working with clay for a little over a year now and my husband and I have decided that commercial glazes are becoming way too expensive. I would like to start experimenting with some engobe decoration.

My question is this, for example, if I am using a porcelain clay body and decide to liquify that same clay body to add a Mason stain to it, wouldn't it be  compatible since the slip/engobe is the same as the clay used to make the piece? I would then mix up a clear coat to apply over the design after bisquing and fire again to make it food safe? I am new to mixing my own glazes and would like to know if anyone knows of a food safe clear coat recipe that is not too glossy, but more of a subtle sheen?

Any advice and help is greatly appreciated. I've been reading many articles and books, but just trying to find the most economical way to proceed with my work. Thanks!

Dora

Views: 694

▶ Reply to This

Replies to This Discussion

Making slips/engobes from your own clay is generally accepted as a good way to go.  You are practically guaranteed a good fit to the body. There is a possibility that unusually large additions of colorants or additives could change the fit, but you are on the right track. What you want to do will give you the cheapest glaze possible.  You could mix up a 45 gallon batch and glaze a small child! There is a 4 ingredient clear on this network that I recommend.

Thanks George for your input! I was hoping I was on the right track. I ordered some stains yesterday and the gentleman at Columbus Clay recommended sodium silicate and frit 3134 to mix in with my slip at approximately 3-5% off each? Thanks for guiding me to the clear glaze recipes. I am creating a recipe book of those I might mix in the near future. This is exciting!

James Chappell's book The Potter's Complete Book of Clay and Glazes is a great resource for learning more about engobes and slips...

ISBN:  0-8230-4203-0

Nadine

dora, have you continued in this search for making your own slips.  I would be interested in knowing how thinks have turned out for you.  I am interested in producing a black slip using mason stain and my cone 6 clay body.  -carl

Hi Carl. I have a cone 10 recipe for a "Metallic Black Slip" If you add the colorants to your clay maybe it would give you a black slip this was from a 100 gram batch. Mang Dioxide 5, iron 4, Cobalt Carb 2, Chrome 2, Copper carb 2, the rest of the slip is Goldart 70, Barnard Clay 15. This was for cone 10. Maybe it is something you could start from. Happy firing and have a great Christmas. 

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service