Is www.Keramik-Kraft.de in Germany the least expensive place to purchase a Type-S thermocouple?

The €95.80 price, roughly $107, is well less than half the price asked by kiln makers and other US vendors I know of.

180 mm long Type-S thermocouple

3 years after installing our Type-S thermocouple it gave use an error message.  I'm hoping cleaning it may fix the problem as it looks intact, but we may need a new one.

Views: 346

▶ Reply to This

Replies to This Discussion

I just needed to clean the dirt and debris off the thermocouple, which must have shorted-out the connection. A problem caused by our studio being outdoors in the open.

So we don't need a replacement Type-S after 3 years of use and 500 to 600 firings.

But I'm still curious where others buy their Type-S thermocouples.

That was a nice find aye? No idea on the TCs. Haven't had to replace one yet. Hopefully I get that kind of result. 

I use type K thermocouples and find the cheaper ones in the USA and very expensive ones at KeramikKraft. 

Best buy for type K was China (< $10). Only tested it in pit fire and bisque firing so far.  Type S, no clue.

Thanks. The accuracy of Type-K is less but acceptable initially. The problem is their inaccuracy increases as they age and the metal crystallizes differently - something thermocouple engineers apparently call "drift".  They end up quite inaccurate prior to the time they fail.

The platinum-rhodium metals in a Type-S are not subject to the cause of drift and last much, much longer. With the number of firings we do, a Type-K lasted 11 to 14 months for us. The Type-S only needed a clean-off of the exterior connections last week after 3 years of use. Due to the fact that we're outdoors and the Type-S use a lower voltage so they're more sensitive to garden debris slightly shorting the connections.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service