Received John Britt's The Complete Guide to Mid-Range Glazes for Christmas - fabulous book and have been enjoying it immensely.  If you have a copy, I have a question.  -  On pg 116, he speaks of making blue glazes by adding stains to a celadon base and on pg 117 shows three tiles (6,7,8) using a glaze called Chun Clear.  Question - Is that the glaze given on pg 81 and called Chun?  If so, would the colorants listed in the glaze recipe (copper carbonate and cobalt carbonate) be left out of the glaze mix to get Chun Clear?  I could not find another reference to Chun Clear in the Index.  Thanks for any help in understanding. 

Views: 542

▶ Reply to This

Replies to This Discussion

I just ordered the book and am looking forward to utilizing it.

I have a recipe from a friend called Chun Clear. How does it compare to the glaze on page 81?

It is:

F4 Soda Feldspar     38

Whiting                    14

Zinc Oxide               12

Ball clay                    6

Silica                       30

exactly the same except chun on pg 81 calls for kaolin instead of ball clay and there is an addition of 0.3 copper carb and 0.3 cobalt carb.  The addition of the carbonates and the fact that the chun on pg 81 is in the list of oxidation celadons makes me think that leaving out the carbonates would be a clear chun.  Sounds like the kaolin is a purer form of clay than the ball clay, but perhaps the ball clay and kaolin are interchangeable in this instance.  I will have the coop studio where I work make up a small batch and see what I get.  Thanks for the input.

I seem to recall a couple of internal references in the book that were hard to follow. With the sheer number of recipes and the extensive commentary concerning various artists results, it is perhaps inevitable that linkages here and there could be missing or unclear. 

Agreed, George. It is an incredible piece of work and I am really enjoying it.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service