Robert spicer's Discussions

Ruined cups

Started this discussion. Last reply by Norm Stuart Apr 17, 2021. 2 Replies

Can someone please tell me why every cup on the left side of the kiln bloated and cracked on the bottom while every cup on the right side of the kiln was perfectly normalcone 05 bisque firing using…Continue

Materials substitution

Started this discussion. Last reply by Norm Stuart Dec 18, 2020. 1 Reply

can Gillespie borate be substituted for gerstley borateContinue

Dry glaze mixing

Started this discussion. Last reply by Jeff Poulter Sep 23, 2015. 3 Replies

The amaco dry glaze mixing instruction suggest 25 lbs of dry material will yield 4 gallons of glaze. Is it safe to assume 25 lbs of dry materials for any glaze recipe will yield roughly the same 4…Continue

Porcelain

Started this discussion. Last reply by Robert spicer Sep 5, 2015. 13 Replies

I fired my first pots thrown with P-5 porcelain and was very disappointed with the results. I had plates warp and bowls go out of round. Having never fired porcelain before I can only guess the kiln…Continue

 

Robert spicer's Page

Latest Activity

Norm Stuart replied to Robert spicer's discussion Ruined cups
"Photos of the fired ware?"
Apr 17, 2021
Robert spicer replied to Robert spicer's discussion Ruined cups
"This was during a cone 05 bisque firing"
Apr 1, 2021
Robert spicer posted a discussion

Ruined cups

Can someone please tell me why every cup on the left side of the kiln bloated and cracked on the bottom while every cup on the right side of the kiln was perfectly normalcone 05 bisque firing using cone 6 stoneware claySee More
Apr 1, 2021
Norm Stuart replied to Robert spicer's discussion Materials substitution
"Yes, gillespie borate will fire very similar to gerstley borate. Each batch of gerstley borate used to be slightly different as they dug through a different area of the deposit."
Dec 18, 2020
Robert spicer posted a discussion

Materials substitution

can Gillespie borate be substituted for gerstley borateSee More
Nov 25, 2020

Profile Information

What is your experience with ceramics in general. (Long answer encouraged)
Started throwing pots in 2010 after visiting Alewine Pottery in Gatlinburg Tn
What is your current involvement with electric fired ceramics? (long answer encouraged)
Own two kilns and am firing constantly
All our content is viewable by the public. Why do you want to be a member, when you can already see everything as a non-member?
Need a network of potters for info and advice about the craft
Where do you work on your ceramics projects?
home studio
How did you find this network?
search engine

Robert spicer's Blog

Pricing of pots

Posted on August 20, 2015 at 7:30pm 2 Comments

Am wondering how potters decide on the worth of their work. I only do 1 show a year and also sell on ETSY. When I look at others work their prices seem to be all over the map. Do you price high and hope to sell items or low in an effort to sell more pieces. I find beautiful vases prices in the $40 to $60 range and next to it is a tea bowl priced at $55. Finding it hard to rationalize the size of the items with their respective prices. Any thoughts?

Comment Wall

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

  • No comments yet!
 
 
 

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service