Started this discussion. Last reply by Norm Stuart Apr 17, 2021. 2 Replies 0 Likes
Can someone please tell me why every cup on the left side of the kiln bloated and cracked on the bottom while every cup on the right side of the kiln was perfectly normalcone 05 bisque firing using…Continue
Started this discussion. Last reply by Norm Stuart Dec 18, 2020. 1 Reply 0 Likes
can Gillespie borate be substituted for gerstley borateContinue
Started this discussion. Last reply by Jeff Poulter Sep 23, 2015. 3 Replies 0 Likes
The amaco dry glaze mixing instruction suggest 25 lbs of dry material will yield 4 gallons of glaze. Is it safe to assume 25 lbs of dry materials for any glaze recipe will yield roughly the same 4…Continue
Started this discussion. Last reply by Robert spicer Sep 5, 2015. 13 Replies 0 Likes
I fired my first pots thrown with P-5 porcelain and was very disappointed with the results. I had plates warp and bowls go out of round. Having never fired porcelain before I can only guess the kiln…Continue
Posted on August 20, 2015 at 7:30pm 2 Comments 0 Likes
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014