C Harris Temoku on Laguna #80 eastern clay
Photo shot in light box with Nikon D3200. 3 - 75 watt halogen bulbs provided lighting.

Views: 105

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Norm Stuart on November 28, 2013 at 8:29pm

There's a lot of available digital display color management software.  Adobe has it built into Photoshop where you enter your make and type of display.

http://www.gballard.net/boutique/colorcorrecting.html

Comment by George Lewter on November 28, 2013 at 7:20pm

I just noticed that on my laptop the color is less saturated than on the desktop. The true color is somewhere between the two renditions. That is something we don't always think about with our various electronic devices -- that the displays vary significantly in how they render color information.


Stars
Comment by Norm Stuart on November 27, 2013 at 10:37pm

I'm sure a company would sell more cameras using a sensor which records richer colors than actually existed.

It's like using KodaChrome in the film era, which people loved because it exaggerated colors.

You can always photograph a reference color chart and create a Photoshop correction filter.

Comment by George Lewter on November 27, 2013 at 11:02am

Thank you! The red in this photo is a bit more saturated than in reality (at least on my screen). Usually I get the opposite - where the photo shows up more brown and the red is hard to discern at all. 


Stars
Comment by Denice E. Demuth on November 27, 2013 at 6:45am

The glaze is very nice, I'm going to put it on my list of glazes to test.  Denice


Stars
Comment by juli long on November 24, 2013 at 10:48am

this glaze looks great!! the pot too!

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service