Nutmeg, Variegated Slate Blue, Water color green, 2-D blue, and Licorice in layers. Has a celadon-like quality with some translucency.

Views: 151

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by juli long on November 2, 2013 at 3:31pm

George,

I love how the glaze broke  on the sweet spots, lip, rim, handle. This is a keeper for sure.

juli

Comment by George Lewter on October 16, 2013 at 5:06pm

Yes, Donna, that is the Water Color Green recipe. Glaze Layers:

  1. Dipped mug in bucket of Nutmeg for a fairly thick coating.
  2. Sprayed Variegated Slate Blue over the Nutmeg medium thickness.
  3. Sprayed Water Color Green over the VSB thinly.
  4. Sprayed 2D Blue to barely cover the other glazes (very thin). 2D Blue is known to make a "snow flake" effect on top of some other glazes if not sprayed too heavily.
  5. Sprayed Licorice on the upper inside and included the rim.

Following are a couple of examples of Nutmeg and Water Color Green from several years ago. I'm not sure,but I'm guessing that I didn't use any Variegated Slate Blue on either of these mugs. The one on the left has been one of my favorite mugs, but the new one above may replace it. 


Stars
Comment by Donna Kat on October 16, 2013 at 3:15pm

Is this it?  The comment says that it is very runny and must be put on thin.  Am I correct that you spray your glazes?


Stars
Comment by Donna Kat on October 16, 2013 at 3:14pm

12) Water Color Green **

Cone 6-10

Custer Feldspar

Flint

Lithium Carb.

3124 Frit

Whiting

Strontium Carb.

Copper Carb.

Bentonite

1440

510

120

150

480

225

240

90


Stars
Comment by Donna Kat on October 16, 2013 at 2:40pm

Is the water color green recipe available?  Beautiful piece.


Stars
Comment by Carl Ray Crutchfield on October 4, 2013 at 6:05pm

beautiful surface glaze, love the contrast

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service