Slip cast bowl with paperclay additions.
Frosty satin matt glaze with Copper carb airbrushed lightly over bowl. Fired to Cone 6 in small electric test kiln.

Views: 147

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by juli long on May 1, 2014 at 7:40am

Jennifer, Thank you for sharing this glaze with me. Here it is on one of my lidded jars on cone 5 brown clay. It has a few pin holes on this clay; not so much on my cone 6 clay. Looks and feels like honed marble. Im still working on amount of coats to put on, and the right amount of water in the bucket! thanks again,

juli

Comment by Jennifer Arthur on December 12, 2013 at 3:44pm

Hi Juli,
This is the recipe.
Enjoy

Frosty Satin Matt Glaze
(Book Greg Daley base glaze E, "Glazing & glazing techniques")

nephiline syenite       60
whiting                        18
talc                             14
kaolin                          18

Airbrushed onto pot
1/2 tspn Copper carbonate
3 tblspn water approx

Mix and spray lightly onto the base glaze.

Comments: Very pretty, maybe thin down the base glaze a little to maintain more detail in the sculptured area.

Comment by juli long on December 12, 2013 at 2:34pm

Jennifer,

This is my favorite bowl of yours.  I love the softness juxtoposed with the barnacle like thingys. I would love the recipe if you are willing to share and post it.

juli

Comment by Denice E. Demuth on September 30, 2013 at 7:18pm

The glaze looks like Milk Glass and the Copper airbrushed on it gives it the look of a really old antique, nice work.  Denice

Comment by juli long on September 30, 2013 at 8:19am

what a cool bowl!!!!

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service