Wheel thrown vase with chatter Celadon ^6 glaze

Views: 595

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by juli long on October 17, 2013 at 4:36pm

" using the High calcium Semi matte Base 2 in theMastering Cone 6 Glazes by Hesselberth and Roy (p-89). Spearmint, Bone, and Raw Sienna are other variations."

This doesnt look semi matte to me. ???


Stars
Comment by Jeff Poulter on October 17, 2013 at 1:00pm

You could also try a smidge of nickel, but nickel doesn't always play nice with TD.  However if you are cutting back on the TD, it might behave itself.  jhp


Stars
Comment by Donna Kat on October 17, 2013 at 11:41am

So a tweak to spearmint then (about half the Cu and Ti and no Fe).  Must be fast cooled as well.  Thank you for that information since I am familiar with spearmint and it looks nothing like this to me.  I had considered adding iron to try and mute it and now know it would not do what I had in mind.  Perhaps a fraction of a percent of cobalt?

Comment by George Lewter on October 16, 2013 at 8:36pm

The recipe for this glaze is one of the color variations using the High calcium Semi matte Base 2 in the Mastering Cone 6 Glazes by Hesselberth and Roy (p-89). Spearmint, Bone, and Raw Sienna are other variations.


Stars
Comment by Donna Kat on October 16, 2013 at 6:58pm

Came across this again and again got fooled again into thinking it was a real celadon.  I am now in position to test it and and am very much looking forward to it. 

Comment by Jeff Morse (Jarrett Pottery) on May 30, 2013 at 6:09am
Donna no problem and it is in oxidation.

Stars
Comment by Donna Kat on May 30, 2013 at 4:57am

Sorry - missed the other comments


Stars
Comment by Donna Kat on May 30, 2013 at 4:57am

Oxidation/Reduction? and would you share the glaze recipe?  Beautiful piece

Comment by Jeff Morse (Jarrett Pottery) on May 25, 2013 at 3:37am
You are very welcome.

Stars
Comment by Nancy Trezza on May 25, 2013 at 3:31am
Jeff-Thanks so much! I'll try it right away!

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service