Potters & Sculptors - Making Rock from Mud
Started Apr 12, 2014 0 Replies 0 Likes
Hi guys,A recently deceased relative left several ceramic slipcast molds, most of which were stored in handmade wooden boxes for the past 35 years.About half of them suited my tastes and preferences,…Continue
Started this discussion. Last reply by Shine Chisholm Dec 28, 2012. 5 Replies 0 Likes
I just started making my own glazes again this year. Before that, it had been about ten years. At that time, Gerstley Borate and Kona F4 Feldspar were still being mined.Many recipes still call for…Continue
Tags: feldspar, minspar, substitions, f4, kona
Started this discussion. Last reply by Brenda Outram Nov 2, 2015. 32 Replies 0 Likes
does anyone have any idea what this beautiful glaze is? I love how it interacts with the clay body.…Continue
Started this discussion. Last reply by Shine Chisholm Oct 31, 2012. 6 Replies 0 Likes
I've been enjoying looking at ceramics on Pinterest, and I'm curious who has a board. I do. It's http://pinterest.com/delicion/I would love to follow you.…Continue
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
Switch to the Mobile Optimized View
© 2025 Created by Andrea Wolf.
Powered by
Comment Wall (3 comments)
You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!
Join Electric Mid&Hi Fired Ceramics
Good day,
I am RonaId Morris, I saw your profile and I decided to contact you immediately. Can you get back to me on my email (ronmorri01@gmail.com) for full details.
Regards.
I'm pleased to meet you!
Hey thanks for commenting on my bowl work. The glaze that's on that work is a crystal glaze, and no, there wasn't recycled glass added. It just happened to be the way the glaze pooled in the middle. It takes a few years to understand how to get it so the glaze doesn't oxide and look funky.
This glaze is rather complex. It involves all aspects of ceramics. The clay body needs to be porcelain, as the glaze is far more brilliant on this clay body. The kiln firing plays a huge role into how this glaze develops. The way you apply it, is another major factor, because this glaze runs. Every where.
The glaze recipe for you, if you wish to work with it:
Ferro Frit 3110
Zinc Oxide
Kaolin
Silica
Lihium Carbonate
and a colorant of your choosing.