Insight-Live User Group

Information

Insight-Live User Group

This is a working group dedicated to testing and sharing glaze research results on our group area of the Insight-Live Glaze Recipe Database. This is absolutely the best place to share your recipes with photos and notes. You can add notes and pictures to other people's recipes showing how your results vary from the originals, and from other people's work with the same glaze. Members are required to periodically contribute notes, pictures, or well documented new recipes to the database.

Videos are available to orient new users with using the database and the user interface, and a text based help system is available

With the online glaze recipe database, members can upload recipes and pictures, search the databases for recipes, append recipes with new notes, and create printable batch mix sheets from recipes. Now members can copy an existing recipe and modify it while comparing the chemistry of both versions.   

This group is the cone6pots portal to Insight-Live. We accept anyone with cone6pots network membership, who agrees to publish photos and/or notes of their results with glaze recipes.. To gain  access to our group's Insight-Live database, you must first join the C6P network, and then this group. Your login information will be generated and sent to you, normally within a day or two.

Database access is a benefit brought to you by supporting members of the cone6pots network.

------------------------------------

Click the button below to login to Insight-Live. When logging in to the group recipe database, type in your user ID, not your email address (which you can use for a different individual account login). If you forget your user ID or password, contact George Lewter and he will send you a new temporary ID/password.

 

Members: 17
Latest Activity: Dec 28, 2019

User Videos for Insight-Live

Tony Hanson has made some excellent user videos for Insight-Live at http://insight-live.com/insight/videos/index.php. If you watch the first couple of them you can begin to appreciate the power of working with glaze chemistry and Insight-Live to tweak your glazes to correct problems and defects.

Specific topics he covers:

A Broken Glaze Meets Insight-Live and a Magic Material (Jan 2013)

Use the calculation mode of Insight-live to make material substitutions for troublesome materials to fix problems like blistering, pinholing, settling and poor slurry and drying properties. Youtube, MP4

How to Use a Lithium Frit in Insight-live (Jan 2013)

Use the calculation mode of Insight-live and non-unity to replace lithium carbonate with a frit. Youtube

Materials and Calculation (Jan 2013)

A tour of the materials management features of Insight-live. MP4

Importing Other File Formats (Oct 2012)

How to import recipe and material data from a wide range of formats. Flash, MP4, M4V

Importing From Generic CSV Spreadsheet (Feb 2013)

You can import data from a sheet having recipe rows and material columns. Youtube

Using Recipe Libraries to transfer recipes to desktop Insight (Mar 2013)

You can export hundreds, even thousands of recipes in a recipe library file. Youtube

Discussion Forum

Should We Stay or Should We Go Now

Started by George Lewter. Last reply by Marina Reijsmeijer (Kleierij) Dec 28, 2019. 16 Replies

Our Insight-live glaze database is not used by many members. I just deleted all members who have not signed in or viewed any recipes since January of 2017. That leaves us with 17 ''active" members.…Continue

Insight expired

Started by Tom Humphries. Last reply by Tom Humphries Oct 23, 2018. 2 Replies

Insight live says my account has expired. Does this mean I've been booted off the group for some reason? :(

Finding the perfect clear

Started by Donna Kat. Last reply by Donna Kat Sep 2, 2018. 7 Replies

Has anyone worked with Tony Hansen's G1214W Clear? I had thought I had found the perfect clear for our studio when I found this glaze. It did not craze on Standard clays. It was crystal clear and it…Continue

My next development project

Started by Arnold Rowntree. Last reply by Jay Decker Mar 23, 2018. 4 Replies

I was searching google images for 'alkaline glazes' and saw this at VVarges page:…Continue

Comment Wall

Comment

You need to be a member of Insight-Live User Group to add comments!

Comment by Sylvia Shirley on February 16, 2012 at 5:01am

I logged in last night on my laptop and spend quite a long time browsing recipes.  It was great.  I did try to use the "email" button to send some to myself, but couldn't get that to work.  I'll try browsing again later with my smartphone.

Reply by George Lewter: I don't think the email function for recipes is implemented yet, but you can set a batch size, and print out a mix sheet. All the info for that glaze except the picture print along with it.

 


Stars
Comment by Don Olliff on February 14, 2012 at 11:56am

I'm having trouble logging into the site. Help...


Stars
Comment by Don Olliff on February 13, 2012 at 3:11pm

Work has been sucking up all my time lately. I finally got some new pieces glazed yesterday. I will try to check in tonight. Not sure my account is setup.

Comment by George Lewter on February 9, 2012 at 5:37am

I tested the batch size feature that Tony added that will recalculate any recipe for whatever total batch size you want. 500 g, 1000, 5000, 7500, 10000.  You can print a mix sheet with all the recalculated amounts.  Very cool!

Comment by George Lewter on January 26, 2012 at 1:40pm

I have made the information contained on the pages for this group viewable by the public, so our activities here will show on the cone6pots main page, and be crawlable by searchbots. This will allow more people to be aware of the work being done on Insight-Live and allow more people to join the group.


Stars
Comment by Tony Hansen on January 25, 2012 at 7:18am
Remember if you want to import as CSV, click the example link on the importer in Insight-Live to see the format it wants. Actually use that as your starting point. If anyone has suggestions on how the format could be more robust, please let me know. Actually, it would be nice if it contained columns for a PictureBaseName.

Stars
Comment by Kathy Ransom on January 24, 2012 at 7:25pm

I've gotten into the database a couple of times but my recipes are all in a scribbler right now so I'm working on getting them into a spreadsheet so I can save them as CSV type and upload them.  I tried for a while on one today but will need to do some more research to figure out where I'm going wrong.  I'm working on my windows based laptop as I have a bit of a learning curve to climb before I try my accessing the database with my phone, Mac, or IPad.

Comment by George Lewter on January 7, 2012 at 5:09pm

We can only do broadcast messages directly from here. To contact a member privately, you need to click their name link or picture icon to go to their profiile page. Once there, in the left column you will see a "Send a Message" link that will open a message editor window.  Once finished, and you click "Send", the message will go to that person's inbox here as well as to their regular email account.

 
 
 

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by