Potters & Sculptors - Making Rock from Mud
This is a working group dedicated to testing and sharing glaze research results on our group area of the Insight-Live Glaze Recipe Database. This is absolutely the best place to share your recipes with photos and notes. You can add notes and pictures to other people's recipes showing how your results vary from the originals, and from other people's work with the same glaze. Members are required to periodically contribute notes, pictures, or well documented new recipes to the database.
Videos are available to orient new users with using the database and the user interface, and a text based help system is available
With the online glaze recipe database, members can upload recipes and pictures, search the databases for recipes, append recipes with new notes, and create printable batch mix sheets from recipes. Now members can copy an existing recipe and modify it while comparing the chemistry of both versions.
This group is the cone6pots portal to Insight-Live. We accept anyone with cone6pots network membership, who agrees to publish photos and/or notes of their results with glaze recipes.. To gain access to our group's Insight-Live database, you must first join the C6P network, and then this group. Your login information will be generated and sent to you, normally within a day or two.
Database access is a benefit brought to you by supporting members of the cone6pots network.
------------------------------------
Click the button below to login to Insight-Live. When logging in to the group recipe database, type in your user ID, not your email address (which you can use for a different individual account login). If you forget your user ID or password, contact George Lewter and he will send you a new temporary ID/password.
Members: 17
Latest Activity: Dec 28, 2019
Tony Hanson has made some excellent user videos for Insight-Live at http://insight-live.com/insight/videos/index.php. If you watch the first couple of them you can begin to appreciate the power of working with glaze chemistry and Insight-Live to tweak your glazes to correct problems and defects.
Specific topics he covers:
A Broken Glaze Meets Insight-Live and a Magic Material (Jan 2013)
Use the calculation mode of Insight-live to make material substitutions for troublesome materials to fix problems like blistering, pinholing, settling and poor slurry and drying properties. Youtube, MP4
How to Use a Lithium Frit in Insight-live (Jan 2013)
Use the calculation mode of Insight-live and non-unity to replace lithium carbonate with a frit. Youtube
Materials and Calculation (Jan 2013)
A tour of the materials management features of Insight-live. MP4
Importing Other File Formats (Oct 2012)
How to import recipe and material data from a wide range of formats. Flash, MP4, M4V
Importing From Generic CSV Spreadsheet (Feb 2013)
You can import data from a sheet having recipe rows and material columns. Youtube
Using Recipe Libraries to transfer recipes to desktop Insight (Mar 2013)
You can export hundreds, even thousands of recipes in a recipe library file. Youtube
Started by George Lewter. Last reply by Marina Reijsmeijer (Kleierij) Dec 28, 2019. 16 Replies 0 Likes
Our Insight-live glaze database is not used by many members. I just deleted all members who have not signed in or viewed any recipes since January of 2017. That leaves us with 17 ''active" members.…Continue
Started by Tom Humphries. Last reply by Tom Humphries Oct 23, 2018. 2 Replies 0 Likes
Insight live says my account has expired. Does this mean I've been booted off the group for some reason? :(
Started by Donna Kat. Last reply by Donna Kat Sep 2, 2018. 7 Replies 0 Likes
Has anyone worked with Tony Hansen's G1214W Clear? I had thought I had found the perfect clear for our studio when I found this glaze. It did not craze on Standard clays. It was crystal clear and it…Continue
Started by Arnold Rowntree. Last reply by Jay Decker Mar 23, 2018. 4 Replies 0 Likes
I was searching google images for 'alkaline glazes' and saw this at VVarges page:…Continue
Comment
thanks , I love this group !!!! :DDD
tengo problemas para entrar al grupo Insight-Live, existe otra manera de entrar , nunca he podido ver los contenidos.
Only after you have uploaded a photo of your test tile or work as an example you can click to "auto-number" the entry as:
C6G - glaze
C6S - slip
C6B - clay body
Clearly the C6 portion is a reference to "Cone 6", but this is overly specific as the database contains recipes for glazes and slips of other cone maturities as well.
If you think we should have codes for glaze attributes beyond what currently exists, please suggest and explain.
These are the current codes available on the left-hand side of the database page under the pink colored tab titled "Our Typecodes"
There needs to exactly one space between each code you enter in the glaze recipe, otherwise Insight-Live doesn't recognize them.
Sorry if I am missing this from somewhere else, I have a question. Did someone take notes or minutes from the Early March type-code skype session? I'm about to input some things that I have useful data on and want to do so properly.
Thanks in advance.
Andrea
Now that we know how "Our Typecodes" work, from tonight's Skype Conference,I made some changes which I think will work better. Example changing Cone 6 Glaze Reduction to three different codes C6 G RX
Each Typecode can be one, two or three letters. As you might expect, the Insight-Live software doesn't care what order you enter attributes, just so long as there's exactly one space between each Typecode.
Comments? Suggestions? Before we get too far . . .
I'll try out Skype for the first time on Thursday if there's a space left.
There is a new group login page at Insight-Live that will help eliminate most sign-in errors.
Save this group sign-in page as a favorite, and you can get into our group database in just two clicks. http://insight-live.com/grouplogin.php
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
Switch to the Mobile Optimized View
© 2025 Created by Andrea Wolf.
Powered by
You need to be a member of Insight-Live User Group to add comments!