Forum Discussions (387)

Discussions Replies Latest Activity

Stars

Green Dragon Matte C6

Green Dragon Matte C6 Cornwall Stone         44 Calcium Carbonate    18 EPK                         3 Zinc Oxide                8 Bentonite…

Started by Jan Wallace in Glazes - Recipe Exchange

0 Apr 11, 2012

SH video is great, recipes firing schedule, Stephen Hill explaining it all...

just received the Stephen Hill Video, wonderful presentation of his method and work. If you purchase the video he sends an updated PDF of…

Started by Tom Waggle in Glazes - Recipe Exchange

3 Mar 21, 2012
Reply by Jan Wallace

Cone 6 firing stuck top

Hi all, I fired this at cone 6. The glaze is firebrick over seaweed sprayed. The problem is the top is stuck on.  The glaze is barely touch…

Started by Randy Clay in Continuing Education

4 Mar 6, 2012
Reply by Donna Ferrara

Floating Blue

I got this recipe from the art center I go to.   This does run some.   and it is figured out in grams for a pretty large batch. I will try…

Started by Carl Ross in Glazes - Recipe Exchange

2 Feb 29, 2012
Reply by Barbara Hanselman

Accounting class Introduction

This class was offered in the Spring of 2012 and completed in early May. It will be offered again, if there is sufficient interest. There w…

Started by George Lewter in Continuing Education

8 Feb 20, 2012
Reply by Beverly Beu Haas

TRANSFER PRINTING FROM PHOTO COPIES TO THE CLAY SURFACE

UPDATED Transfer Print-to-pot Musings… Some of you are already aware that you can use grease pencils or Crayola crayons to make designs or…

Started by Barbara Hanselman in Altering and Decorating Forms

0 Feb 18, 2012

Why Are We Here? What This Network Is, and What It Could Be.

Almost two year ago, I started the cone6pots network, as I started getting back into pottery in a serious way. I could have been satisfied…

Started by George Lewter in Network User Guide

17 Feb 13, 2012
Reply by Jan Wallace

How to turn your pottery knowledge into a business

Lakeside Pottery is a ceramic art teaching facility in Stamford, CT with over 4,500 enrolments in the past 7 1/2 years. We have experianced…

Started by Morty Bachar in Marketing & Business Savvy

1 Feb 3, 2012
Reply by Benjamin Coffman

Stars

Jan Wallace Cone 6 Test Results

Below are the results from my first batch of Cone 6 tests. I collected a number of glaze recipes, alot from this site and from other source…

Started by Jan Wallace in Glazes - Testing and Reporting

14 Feb 1, 2012
Reply by Benjamin Coffman

Stars

Underglazes can go on leather up to bone dry?f

I see no-one has started a thread in this section yet, so I'll make my very first post as a novice.  I'm most interested in sgraffito techn…

Started by Rebekah Ross in Altering and Decorating Forms

4 Feb 1, 2012
Reply by Patricia

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by