Amaco High Fire Glazes

I am experimenting with some interesting construction techniques and have been using Amaco high fire white because it can be used on greenw…

Started by Marla Stroup in Commercial Glazes

13 Aug 7, 2014
Reply by Marti Howell

Stars

Rutile - is natural material art, or just a challenge to artists?

Below is the "^6 Honey" glaze made with a ten year old bag of Dark Rutile from Laguna Clay compared with: 1.)  Dark Rutile from U.S. Pigmen…

Started by Norm Stuart in Glazes - Development and Adjustment

0 Aug 4, 2014

Talc versions at Aardvark

I am just starting to put my first order together for raw materials for cone 6. The online catalog at Aardvark lists 3 different Talcs: Tal…

Started by Darthe Hues in Ceramic Materials Education

7 Aug 4, 2014
Reply by Darthe Hues

Stars

Repairing a bisque ware.

Not really a glaze question. However would really like to know if one can repair a crack (not a S crack) in a bisqued platter with paper cl…

Started by Srirupa Sen in Network User Guide

4 Jul 29, 2014
Reply by Norm Stuart

Adjustable Slab Slump Molds

I just got my rectangular mold in the mail today, and I am a happy camper. I got a chance to try one last winter at MIY Ceramics and Glass…

Started by George Lewter in Pottery Equipment

0 Jul 26, 2014

Stars

Single fire a sculpture?

Please let me know if these sounds like a good idea. (1)I made this dragon he's in greenware stage I'm thinking of spraying him with greens…

Started by Karen Mandeville in Network User Guide

4 Jul 24, 2014
Reply by George Lewter

Stars

Couldn't have done it without this site!

Just want to say thank you to all the people who have shared glaze recipes! I have tested many, and just wanted to show and tell!

Started by juli long in Glazes - Testing and Reporting

10 Jul 20, 2014
Reply by juli long

Time-sensitive question: Rutile wash + colored slip

I'm still in the learning stage re using rutile. First question: Can two bowls that have a cobalt oxide-colored slip plus an added rutile w…

Started by Meredith Walker in Network User Guide

5 Jul 18, 2014
Reply by Norm Stuart

opulence matt base question

I have been gifted 25 lb's(dry) of Opulence matt base(cone 6). and am wondering what are some of the amts of coloring oxides/carbonates and…

Started by Wyndham Dennison in Commercial Glazes

3 Jul 13, 2014
Reply by Wyndham Dennison

Stars

Digital Scales

My triple beam scales have cratered on me, so I'm in the market for some digital scales.  I hope someone is  using scales that they could r…

Started by Denice E. Demuth in Pottery Equipment

21 Jul 10, 2014
Reply by Jacob Smith

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service