I am experimenting with some interesting construction techniques and have been using Amaco high fire white because it can be used on greenware and also bisque fired pieces.

The colors are not very appealing though and I will have to run test tiles of course but was just wondering if anyone has had any luck in layering or otherwise mixing any of these glazes from the High fire group?

Some are in a collection called Sabara Liquid Glazes and another HF Series is called Celebration Liquid Glazes. I just knew them as "High Fire" since their numbers were HF 11, HF 17,  etc.

Views: 2223

▶ Reply to This

Replies to This Discussion

Thanks for the tip on checking each glaze. If you order online there is no way to do that unless you ask the seller to do it before purchase. I only have 2 Sahara glazes: the Oatmeal & Textured Tan. I like the oatmeal but will probably add some yellow stain to it & see what happens. It IS a pretty matt glaze & will cover very dark clay. I don't care for the Tan at all. They both say "greenware", so you could be right. The only time I've seen glaze used on greenware was when I was doing some firing for a pottery studio & some people were putting Duncan Concepts on their pieces. You might look into that - also Mayco Stroke & Coat which comes in bright colors & some (it says on the bottle) are very stable at ^5. Go on Mayco's website & find their high fire PDF. They list all their glazes & what happens to them fired at ^5. VERY HELPFUL!

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service