Forum Discussions (387)

Discussions Replies Latest Activity

Scheduling slow-cool cycles after you have reached temp

Hi all - I did not schedule a slow cooling cycle when I fired the kiln, but decided after it had reach temp that I wanted to try it.  Is th…

Started by Ian Hall-Hough in Firing Techniques

5 Mar 10, 2016
Reply by Jeff Poulter

Blender 3-d Software for Design and 2-d Pattern Making

If you've tried to make slab objects from patterns, you know how hard it is to get the pattern just right to create the shape you are thin…

Started by George Lewter in Altering and Decorating Forms

1 Mar 4, 2016
Reply by Erik Evans

looking for a nice running glaze

does anyone have a recipe for a base running glaze?  Yes, I know we all try hard to avoid this, but I'd like something to drip over the rim…

Started by Ginny Waters in Glazes - Recipe Exchange

7 Feb 2, 2016
Reply by Jon Butler

Special Effects with Brush Application

Brushing glazes seems so basic that we seldom discuss it.  It just isn't sexy.  But I have spent the past year finding ways to make my brus…

Started by Dawn Atkin in Glazes - Application Techniques

16 Jan 26, 2016
Reply by George Lewter

Stars

Home grown Kiln controller

Hi Cone sixers: I am working on a Java based ceramic kiln controller. I have a proto roughed out that works through an Arduino and a solid…

Started by Robert Coyle in Pottery Equipment

12 Jan 13, 2016
Reply by Marina Reijsmeijer (Kleierij)

Iron Glazes and Achieving Red Color in Oxidation

Following is an extract from John Sankey's Website with detailed instructions on achieving iron reds.Summary Red iron oxide Fe2O3 decompose…

Started by George Lewter in Glazes - Development and Adjustment

3 Jan 8, 2016
Reply by juli long

Spraying Glazes - A good starter compressor and spray gun set?

I see a lot of beautiful work done by people spraying glazes. I have only been brushing and dipping for a long time now and I am ready to m…

Started by Joseph Fireborn in Glazes - Application Techniques

2 Dec 26, 2015
Reply by Joseph Fireborn

Stars

Slip and Hakeme Decoration

Been reading a lot about Jim Malone, Mike Dodd, and to some extent Phil Rogers regarding treatment with slip using finger trailing or Hakem…

Started by cp dunbar in Glazes - Development and Adjustment

0 Dec 14, 2015

Firing pots with lids on

I recently did a bisque firing and had problems with cracking of my small storage jars. They didn't actually fall apart, but cracks are cle…

Started by Tom Humphries in Firing Techniques

3 Nov 4, 2015
Reply by Norm Stuart

What is this glaze?

does anyone have any idea what this beautiful glaze is? I love how it interacts with the clay body.

Started by Shine Chisholm in Glazes - Recipe Exchange

32 Nov 2, 2015
Reply by Brenda Outram

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service