Do I need to poke a hole in this double wall bowl? The lid has a thrown hollow knob that I poke a small hole in, and a rolled rim, that I don't poke a hole in. I am not sure if I need to poke a hole some where in the double walled bowl. 

Views: 271

▶ Reply to This

Replies to This Discussion

hope these pic. show

Attachments:

Yes otherwise it may crack when it dries. The air on the inside will be trapped and as the clay shrinks it will have no where to go and make its own hole to escape!

I think an even bigger issue would be during firing as the expanded air tries to make its way out through the maturing body and glaze. 

I just made another one and cut it into to get a better look. I was thinking …to wait to poke, until leather hard, but after reading y'alls replies, I will find a way to poke a hole before it starts to dry.  Maybe two holes to be safe!

Thanks so much for the quick responses!

I needed them.

juli

my double wall jewelry bowls survived the firings with no problems.  I glazed the outside thin with metallic green to get an orange tone, and added glass in the center and on the lid. I trimmed the bottom open so not to trap air, and glazed inside the trimmed area as well.  These are small and hold rings and earrings.

Attachments:

jewelry bowls


this is how I trimmed them.  I made the opening at the bottom and glazed inside this area as well, otherwise it would have been a solid bottom with trapped air.
juli long said:

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service