Daniel Spruyt's Discussions (37)

Discussions Replied To (27) Replies Latest Activity

"Thank you for the interest. "

Daniel Spruyt replied May 11, 2014 to Can one predict the appearance of a glaze? (part I: The Si/Al ratio)

9 Oct 19, 2016
Reply by Tom Humphries

"That is the range in which the glazes are glossy (best melt, close to eutectic) "

Daniel Spruyt replied May 10, 2014 to Can one predict the appearance of a glaze? (part I: The Si/Al ratio)

9 Oct 19, 2016
Reply by Tom Humphries

"I continue the discussion with some examples of recent sandblasting results. In the…"

Daniel Spruyt replied May 8, 2014 to Sandblasting

3 May 8, 2014
Reply by Daniel Spruyt

"Hi Larry, No, this sand often used for masonry is much too coarse for the air eraser…"

Daniel Spruyt replied May 8, 2014 to Sandblasting

3 May 8, 2014
Reply by Daniel Spruyt

"Another alternative to water etching is sand blasting. I have little experience yet,…"

Daniel Spruyt replied Apr 19, 2014 to Water etching

25 May 26, 2014
Reply by Daniel Spruyt

"There are magnificent examples of water etched ceramics on the Internet. Arne Ase is…"

Daniel Spruyt replied Apr 19, 2014 to Water etching

25 May 26, 2014
Reply by Daniel Spruyt

"Hi Carolyne, Personally, I don't like wax or wax solutions much. I tried them as res…"

Daniel Spruyt replied Apr 19, 2014 to Water etching

25 May 26, 2014
Reply by Daniel Spruyt

"I think carving is much more tedious and time consuming - at least for detailed desi…"

Daniel Spruyt replied Apr 18, 2014 to Water etching

25 May 26, 2014
Reply by Daniel Spruyt

"Thanks for the interest and compliment. Regarding ceramic works in big cities: No, w…"

Daniel Spruyt replied Apr 16, 2014 to Chemistry in Ceramics

2 Apr 16, 2014
Reply by Daniel Spruyt

"The actual setup is not available for download. It is the work of years of developme…"

Daniel Spruyt replied Apr 16, 2014 to Keeping record of your work

2 Apr 16, 2014
Reply by Daniel Spruyt

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014